Grade : | X6CrNiTiB18-10 | ||||||
Number: | 1.4941 | ||||||
Classification: | Austenitic creep resisting steel | ||||||
Density: | 7.9 g/cm ³ | ||||||
Standard: |
|
Ti = 5 * C to 0.8 |
C | Si | Mn | Ni | P | S | Cr | Ti | B |
0.04 - 0.08 | max 1 | max 2 | 9 - 12 | max 0.035 | max 0.015 | 17 - 19 | max 0.8 | 0.0015 - 0.005 |
Rm - Tensile strength (MPa) (+A) | 490-710 |
Rm - Tensile strength (MPa) (+AT) | 490-690 |
Rp0.2 0.2% proof strength (MPa) (+A) | 200-220 |
Rp0.2 0.2% proof strength (MPa) (+AT) | 175-195 |
KV - Impact energy (J) transverse, (+A) | +20° 60 |
KV - Impact energy (J) longitud., (+A) | +20° 100 |
A - Min. elongation at fracture (%) (+A) | 40 |
A - Min. elongation at fracture (%) (+AT) | 30-40 |
Resistance to intergranular corrosion: in the delivery condition - yes; in the sensitized condition - yes (EN 10028-7). ??? Resistance to intergranular corrosion -no (EN 10216-5) |
EU EN | France AFNOR | |
X6CrNiTiB18-10 |
|