1.4571 Steel Plate flange EN1092-1 TYPE 01 Steel Material : X6CrNiMoTi17-12-2
Grade : | X6CrNiMoTi17-12-2 |
Number: | 1.4571 |
Classification: | Austenitic stainless steel |
Density: | 8 g/cm ³ |
Standard: | EN 10088-2: 2005 Stainless steels. Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes | EN 10088-3: 2005 Stainless steels. Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes | EN 10028-7: 2007 Flat products made of steels for pressure purposes. Stainless steels | EN 10222-5: 2000 Steel forgings for pressure purposes. Martensitic, austenitic and austenitic-ferritic stainless steels | EN 10216-5: 2014 Seamless steel tubes for pressure purposes. Technical delivery conditions. Stainless steel tubes | EN 10217-7: 2005 Welded steel tubes for pressure purposes. Stainless steel tubes | EN 10296-2: 2005 Welded circular steel tubes for mechanical and general engineering purposes. Stainless steel. Technical delivery conditions | EN 10253-3: 2008 Butt-welding pipe fittings. Wrought austenitic and austenitic-ferritic (duplex) stainless steels without specific inspection requirements | EN 10253-4: 2008 Butt-welding pipe fittings. Wrought austenitic and austenitic-ferritic (duplex) stainless steels with specific inspection requirements | EN 10272: 2007 Stainless steel bars for pressure purposes | EN 10263-5: 2001 Steel rod, bars and wire for cold heading and cold extrusion. Technical delivery conditions for stainless steels | EN 10250-4: 2000 Open steel die forgings for general engineering purposes. Stainless steels | EN 10297-2: 2005 Seamless circular steel tubes for mechanical and general engineering purposes. Stainless steel. Technical delivery conditions | EN 10088-1: 2005 Stainless steels. List of stainless steels | EN 10088-5: 2009 Stainless steels. Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels for construction purposes | EN 10088-4: 2009 Stainless steels. Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for construction purposes | |
1.4571 Steel Plate flange Chemical composition % of steel X6CrNiMoTi17-12-2 (1.4571): EN 10088-2-2005
Ti = 5 * C to 0.7 Particular ranges of sulphur content may provide improvement of particular properties. For machinability a controlled sulphur content of 0.015 % to 0.030% is recommended and permitted. For weldability, a controlled sulphur content of 0.008 % to 0.030 % is recommended and permitted. For polishability, a controlled sulphur content of 0.015 % max is recommended. Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast. |
C | Si | Mn | Ni | P | S | Cr | Mo | Ti |
max 0.08 | max 1 | max 2 | 10.5 - 13.5 | max 0.045 | max 0.015 | 16.5 - 18.5 | 2 - 2.5 | max 0.7 |
1.4571 Steel Plate flange Mechanical properties of steel X6CrNiMoTi17-12-2 (1.4571)
Rm - Tensile strength (MPa) (+A) | 500-700 |
Rm - Tensile strength (MPa) (+AT) | 500-730 |
Rm - Tensile strength (MPa) (+AT+C) | 810-850 |
Rp0.2 0.2% proof strength (MPa) (+A) | 200-240 |
Rp0.2 0.2% proof strength (MPa) (+AT) | 190-210 |
KV - Impact energy (J) transverse, (+A) | +20° 60 | -196° 60 |
KV - Impact energy (J) longitud., (+A) | +20° 100 |
A - Min. elongation at fracture (%) (+A) | 30-40 |
A - Min. elongation at fracture (%) longitud., (+AT) | 35-45 |
Nominal diameter (mm): | 2 - 50 |
Z - Reduction in cross section on fracture (%) | 60-65 |
Brinell hardness (HB): (+A) | 215 |
Brinell hardness (HB): (+AT) | 210 |