Grade : | S355J0H | ||
Number: | 1.0547 | ||
Classification: | Non-alloy structural steel | ||
Standard: |
|
Method of deoxidation FN = rimming steels not permitted CEV < 0.45 / 0.53 for thickness 16 / 65 mm |
C | Si | Mn | P | S | N |
max 0.22 | max 0.55 | max 1.6 | max 0.035 | max 0.035 | max 0.009 |
Nominal thickness (mm): | to 3 | 3 - 100 | 100 - 120 |
Rm - Tensile strength (MPa) | 510-680 | 470-630 | 450-600 |
Nominal thickness (mm): | to 16 | 16 - 40 | 40 - 63 | 63 - 80 | 80 - 100 | 100 - 120 |
ReH - Minimum yield strength (MPa) | 355 | 345 | 335 | 325 | 315 | 295 |
KV - Impact energy (J) | 0° 27 |
Nominal thickness (mm): | to 40 | 40 - 63 | 63 - 100 | 100 - 120 |
A - Min. elongation at fracture (%) longitud., | 22 | 21 | 20 | 18 |