2. alloys UNS N06002, UNS N06230, UNS N12160, and UNS R30556* in the form of rod for heat resisting and general-corrosive service
Composition Limits, %
UNS N06002 UNS N06230 UNS N12160 UNS R30556
Nickel remainderA remainderA remainderA 19.0–22.5
Iron 17.0–20.0 3.0 max 3.5 max remainderA
Chromium 20.5–23.0 20.0–24.0 26.0-30.0 21.0–23.0
Cobalt 0.5–2.5 5.0 max 27.0-33.0 16.0–21.0
Molybdenum 8.0–10.0 1.0–3.00 1.0 max 2.5–4.0
Tungsten 0.2–1.0 13.0–15.0 1.0 max 2.0–3.5
Carbon 0.05–0.15 0.05–0.15 0.15 max 0.05–0.15
Silicon 1.00 max 0.25–0.75 2.4-3.0 0.20–0.80
Manganese 1.00 max 0.30–1.00 1.5 max 0.50–2.00
Phosphorus 0.04 0.030 max 0.030 max 0.04 max
Sulfur 0.03 0.015 max 0.015 max 0.015 max
Columbium ... ... 1.0 max 0.30 max
Tantalum ... ... ... 0.30–1.25
Aluminum ... 0.20–0.50 ... 0.10–0.50
Zirconium ... ... ... 0.001–0.10
Lanthanum ... 0.005–0.050 ... 0.005–0.10
Nitrogen ... ... ... 0.10–0.30
Boron ... 0.015 max ... 0.02 max
Mechanical Property Requirements
UNS
Tensile
Strength, min,
ksi (MPA)
Yield Strength
(0.2 % Offset),
min, ksi (MPa)
Elongation in
2 in. (50.8
mm) or 4DA
min, %
N06002 95 (660) 35 (240) 35
N06230B 110 (760) 45 (310) 40
N12160C 90 (620) 35 (240) 40
R30556D 100 (690) 45 (310) 40
----------Accept The 3rd Party (SGS/TUV/BV, etc) TO TEST
3. size 7.94~88.9mm diameter
4. surface pickled,Lathe polished,descaling,black,bright, acid-producing white,drawn-bright
5. Packing: steel strip or wooden cases
6. Lead time: 10~30days according to qty
7. Test: in-house or the 3rd party to test (SGS,TUV,BV,etc)