Stainless Steel Seamless Pipe, ASTM A312 TP316Ti , B16.10 & B16.19, , 6M ,PE / BE, HOT FINISHED SURFACE
Standard Specification:
ASTM A213 / A213M - 11a:Standard Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes
ASTM A269 - 10:Standard Specification for Seamless and Welded Austenitic Stainless Steel Tubing for General Service
ASTM A312 / A312M - 12:Standard Specification for Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes
ASTM A511 / A511M - 12:Standard Specification for Seamless Stainless Steel Mechanical Tubing
ASTM A789 / A789M - 10a:Standard Specification for Seamless and Welded Ferritic/Austenitic Stainless Steel Tubing for General Service
ASTM A790 / A790M - 11:Standard Specification for Seamless and Welded Ferritic/Austenitic Stainless Steel Pipe
DIN 17456-2010:GENERAL PUROSE SEAMLESS CIRCULAR STAINLESS STEEL TUBES.
DIN 17458-2010:Seamless Circular of Austenitic Stainless Steel Tube
EN10216-5 CT 1/2 : Stainless Steel Seamless Pipe & Tube
GOST 9941-81:SEAMLESS COLD- AND WARM-WORKED TUBES MADE OF CORROSION RESISTANT STEEL.
Others like BS, JIS standard or can supply
Material Grade:
American Standard | Austenitic Steel: TP304,TP304L,TP304H, TP304N, TP310S,TP316,TP316L,TP316Ti,TP316H, TP317,TP317L, TP321, TP321H,TP347, TP347H,904L… Duplex Steel : S32101,S32205,S31803,S32304,S32750, S32760 Others:TP405,TP409, TP410, TP430, TP439,... |
Europen Standard | 1.4301,1.4307,1.4948,1.4541,1.4878,1.4550,1.4401,1.4404,1.4571,1.4438, 1.4841,1.4845,1.4539,1.4162, 1.4462, 1.4362, 1.4410, 1.4501 |
Russia Standard | 08Х17Т,08Х13,12Х13,12Х17,15Х25Т,04Х18Н10,08Х20Н14С2, 08Х18Н12Б,10Х17Н13М2Т,10Х23Н18,08Х18Н10,08Х18Н10Т, 08Х18Н12Т,08Х17Н15М3Т,12Х18Н10Т,12Х18Н12Т,12Х18Н9, 17Х18Н9, 08Х22Н6Т, 06ХН28МДТ. |
Size Range:
Production | Outside Diameter | Wall Thickness |
Seamless Pipe | 6.00mm to 850mm | 0.5mm to 52mm |
Final Finishing:
Solution Annealed & Pickled
This grade is particularly useful in control and instrumentation tubing applications where 316 and 317L are not suitable.
Temper | Annealed | |
---|---|---|
Tensile Rm | 71 | ksi (min) |
Tensile Rm | 490 | MPa (min) |
R.p. 0.2% Yield | 32 | ksi (min) |
R.p. 0.2% Yield | 220 | MPa (min) |
Elongation (2” or 4D gl) | 35 | % (min) |
Specific Heat (0-100°C) | 450 | J.kg-1.°K-1 |
Thermal Conductivity | 11.5 | W.m -1.°K-1 |
Thermal Expansion | 15.8 | mm/m/°C |
Modulus Elasticity | 190 | GPa |
Electrical Resistivity | 9.52 | μohm/cm |
Density | 7.95 | g/cm3 |
Element | Min | Max |
---|---|---|
C | - | 0.2 |
Mn | - | 2 |
Ni | 23 | 28 |
Cr | 19 | 23 |
S | - | 0.3 |
Mo | 4 | 5 |
N | - | 0.1 |
Cu | 1 | 2 |
P | - | 0.03 |
Si | - | 0.7 |