316L Stainless Steel Plate DIN1.4404 Metal Plate Laser Cutting and Bending
16 / 316L are austenitic stainless steels that contain molybdenum, which increases their resistance to many chemical corrodents and marine environments. 316L is an extra low carbon version of 316 stainless steel. These materials are more resistant to general corrosion and pitting/crevices than conventional austenitic stainless steels. They also offer higher creep, stress-to-rupture and tensile strength at elevated temperatures, excellent corrosion resistance and strength properties, and they are well suited for fabricated or formed applications.
Please contact us for more details.
The technical data provided is for information only and not for design purposes. It is not warranted or guaranteed.
For a deeper understanding of the difference between 304 and 316, request our white paper on the topic.
Element | Percent by Weight | |
---|---|---|
316 Stainless | ||
C | Carbon | 0.08 max |
Mn | Manganese | 2.00 max |
Si | Silicon | 0.75 max |
Cr | Chromium | 16.00 - 18.00 |
Ni | Nickel | 10.00 - 14.00 |
Mo | Molybdenum | 2.00 - 3.00 |
P | Phosphorus | 0.045 max |
S | Sulfur | 0.030 max |
N | Nitrogen | 0.10 max |
Fe | Iron | Bal. |
Element | Percent by Weight | |
---|---|---|
316L Stainless | ||
C | Carbon | 0.030 max |
Mn | Manganese | 2.00 max |
Si | Silicon | 0.75 max |
Cr | Chromium | 16.00 - 18.00 |
Ni | Nickel | 10.00 - 14.00 |
Mo | Molybdenum | 2.00 - 3.00 |
P | Phosphorus | 0.045 max |
S | Sulfur | 0.030 max |
N | Nitrogen | 0.10 max |
Fe | Iron | Bal. |
Temperature Range | Mean Coefficient of Thermal Expansion | ||
---|---|---|---|
°C | °F | cm/cm/°C | in/in/°F |
20 - 100 | 68-212 | 16.5 · 10-6 | 9.2 · 10-6 |
20 - 500 | 68-932 | 18.2 · 10-6 | 10.1 · 10-6 |
20 - 1000 | 68-1832 | 19.5 · 10-6 | 10.8 · 10-6 |
Temperature Range | W/m · K | Btu/(hr/ft²/in/°F) | |
---|---|---|---|
°C | °F | ||
20-100 | 68-212 | 14.6 | 100.8 |
°C | °F | J/kg °K | Btu/lb/°F |
---|---|---|---|
20 | 68 | 450 | 0.108 |
93 | 200 | 450 | 0.116 |
Type | Value at 68°F (20°C) | |
---|---|---|
Microhm-cm | MIcrohm-in. | |
316 | 29.1 | 74.0 |
Property | Type 316 (S31600) | Type 316L (S31603) | Type 317 (S31700) | Type 317L (S31703) |
---|---|---|---|---|
Yield Strength 0.2% Offset psi MPa | 30,000 205 | 25,000 170 | 30,000 205 | 30,000 205 |
Ultimate Tensile Strength psi MPa | 75,000 515 | 70,000 485 | 75,000 515 | 75,000 515 |
Percent Elongation in 2 in. or 51mm | 40.0 | 40.0 | 35.0 | 40.0 |
Hardness, Max. Brinell RB | 217 95 | 217 95 | 217 95 | 217 95 |