Nickel Pipe Inconel 800 series UNS S08811 Inconel 800 800H 800Ht Nickel Tube & Pipe
Nickel and Nickel alloy referred to the alloy’s main elemental contents of Ni, Cu, Cr, Fe and Mo.
Those all characterized by its combination performance of high corrosion resistance and heat ability at temperature 650 ~ 1000 °C.
According to main alloy elements content can divide:
Ni –Cr – Mo alloy (Inconel 600 Series)
Ni-Cr-Fe alloy (Incoloy 800 Series)
Ni - Mo – Ni – Cu – (Hastelloy Series)
Pure Nickel and low alloy nickel (Nickel 200/201)
Application:
- High temperature process
- Chemical and Petrochemical field
- Food field
- Power plants
Material List:
Incoloy 800, Incoloy 800H, Incoloy 825, Inconel 600, Hastelloy B, Hastelloy B2, Hastelloy C, Hastelloy C276,
Hastelloy C4, Hastelloy C22, Inconel 625, Inconel 718, Monel 400, Nickel 200
Inconel 800 Series
Alloy 800 (UNS N08800), Alloy 800H (UNS 08810) and alloy 800AT (UNS N08811) have the same content of Nickel, Chromium and iron, what makes the difference is the combined titanium and aluminium levels (0.85 to 1.2%) to ensure optimum high temperature properties.
Chemical Composition:
Alloy | Ni | Cr | Fe, Min | C, Max | Al | Ti | Al+Ti |
Alloy 800 | 30-35 | 19-23 | 39.5 | 0.10 | 0.15-0.60 | 0.15-0.60 | 0.30-1.20 |
Alloy 800H | 30-35 | 19-23 | 39.5 | 0.05-0.10 | 0.15-0.60 | 0.15-0.60 | 0.30-1.20 |
Alloy 800HT | 30-35 | 19-23 | 39.5 | 0.06-0.10 | 0.25-0.60 | 0.25-0.60 | 0.85-1.20 |
Mechanical Property:
Density, g/m2 | 7.94 |
Melting range, °C | 1357~1385 |
Tesile Strength, Min , Mpa | 550 |
Yield Strength, Min , Mpa | 240 |
Elongation, % , Min | 30 |
Hastelloy C22 | Inconel 600 | Inconel 625 | Inconel 718 |
Inconel 800 | Nickel 200 | Nickel 400 | Nickel alloy C276 |