AlSr Al-10Sr Al-15Sr Aluminum Strontium alloy ingot rod coil master alloy
AlSr10 aluminum strontium alloy modifier Purpose: Al-Sr is applicable to metal casting, low pressure casting and hypoeutectic and eutectic aluminum silicon alloy modification with long casting time.
Usage
After finishing alloying, Keep the temperature at 730-745°C and then put the aluminum strontium alloy in it for 10 mins, mix and refine fully for another 10 mins with high-purity nitrogen or argon gas, finally anneal for 25 Minutes is ok.
Packing
SEAWORTHY PACKING, VACUUM PACKING, PLASTIC FILM PACKED AND PUT INTO IRON DRUM WITH VACUUM. ALSO AS CLIENTS' REQUIREMENT.
Magnesium basis master alloy: MgCa,MgMn,MgY,MgSr,MgZr,MgGd,MgSc etc.
Aluminum basis master alloy:AlSr, AlTi,AlCu,AlV,AlSr,AlZr,AlMn,AlSc etc.