Advantages/Benefits
▪ Excellent mortar bonding ensures highest loads in
concrete.
▪ Suitable for underwater installations.
▪ Suitable for diamond drilled holes.
▪ Expansion-free anchoring allows low axial spacings and
edge distances.
Our main product series
-- Concrete repair system
XQ-GF crack grouting adhesive
XQ-FF crack sealing adhesive
-- Steel bonding reinforcement system
XQ-JGN structural epoxy adhesive
XQ-GZ Grouting epoxy adhesive
XQ-FB edge sealing adhesive
-- Chemical Anchor series
Pure Epoxy Adhesive 360ml (5:1) 390ml(3:1) 585ml (3:1)
-- Carbon fiber reinforcement system,
XQ-XW carbon fiber epoxy adhesive
XQ-XB concrete surface leveling epoxy adhesive
XQ-CFC carbon fiber fabric 12K unidirectional 200gsm-600gsm
Testing project | Condition | Index | ||
Gel Performance (According to China National Standard GB50728-2011) | ||||
Splitting Tensile Strength (MPa) | Under (23±2)℃,(50±5)%RH, tested by loading speed of 2mm/min | ≥8.5 | ||
Flexural Strength (MPa) | ≥50 (no fragment damage) | |||
Compressive Strength (MPa) | ≥60 | |||
Bonding Capacity (According to China National Standard GB50728-2011) | ||||
Steel-Steel Tensile Shear Strength (MPa) | (23±2)℃,(50±5)%RH | ≥10 | ||
Bonding strength of Ribbed steel bar (or screw) with concrete under constrain drawing condition | (23±2)℃ (50±5)%RH | C30,Ф25,L=150mm | ≥11 | |
C60,Ф25,L=150mm | ≥17 | |||
Steel-Steel T-peeling strength (mm) | (23±2)℃,(50±5)%RH | ≤25 | ||
Non-volatile content | (105±2)℃,(180±5)min | ≥99% | ||
Ageing resistance to heat and humidity 90d | ||||
Reduction rate of tensile strength | Under normal room temperature | ≤12% | ||
(According to China National Standard JGJ145-2013) | ||||
Tensile Strength (after high temperature welding) | Dia12 Grade II steel, C30 concrete Hole dia.16mm, Depth: 150mm | 55.1N, 57.0N, 54.8N |