C
|
Mn
|
Si
|
P
|
S
|
Cr
|
Mo
|
Ni
|
N
|
2205 (S31803)
|
0.03
|
2.0
|
1.0
|
0.03
|
0.02
|
21.0- 23.0
|
2.5-3.5
|
4.5-6.5
|
0.08-0.20
|
2205 (S32205)
|
0.03
|
2.0
|
1.0
|
0.03
|
0.02
|
22.0-23.0
|
3.0-3.5
|
4.5-6.5
|
0.14-0.20
|
Grade
|
Tensile Strength ksi (min)
|
Yield Strength 0.2% ksi (min)
|
Elongation %
|
Hardness (HB) MAX
|
2205
|
90
|
65
|
25
|
217
|
|
Density
lbm/in3 |
Electrical
Resistivity mW•in |
tdermal
Conductivity (BTU/hr•ft•°F) |
Heat
Capacity BTU/lbm•°F |
Electrical
Resistivity (in x 10-6) |
at 68°F
|
0.278
|
27.6
|
8.7
|
0.112
|
33.5
|
at 212°F
|
|
26.1
|
9.2
|
0.119
|
35.4
|
at 392°F
|
|
25.4
|
9.8
|
0.127
|
37.4
|
at 572°F
|
|
24.9
|
10.4
|
0.134
|
39.4
|
|
Ni
|
Cr
|
Mo
|
Mn
|
Si
|
C
|
N
|
S
|
P
|
Fe
|
MIN
|
4.5
|
22.0
|
3.0
|
-
|
-
|
-
|
0.14
|
-
|
-
|
-
|
MAX
|
6.5
|
23.0
|
3.5
|
2.0
|
1.0
|
0.03
|
0.2
|
0.02
|
0.03
|
Balance
|
Temperature, °F
|
70
|
212
|
392
|
572
|
Coefficient* of Thermal Expansion, in/in°F x 10-6
|
-
|
8
|
8
|
8
|
Thermal Conductivity
Btu • ft/ft2 • hr • °F |
8
|
9
|
10
|
11
|
Modulus of Elasticity, Dynamic psi x 106
|
28
|
26
|
25
|
24
|
Mechanical Properties
Ultimate Tensile Strength, ksi
|
95
|
0.2% Yield Strength, ksi
|
65
|
Elongation, %
|
25
|
Hardness MAX, Brinell
|
290
|
Temperature, °F | 212 | 302 | 392 | 482 |
Ultimate Tensile Strength, ksi | 86 | 83 | 80 | 78 |
0.2% Yield Strength, ksi | 52 | 49 | 46 | 44 |
|
PREn
|
Critical Pitting Temperature, CPT
|
2205
|
34
|
130°F
|
316L
|
24
|
62°F
|