Cobalt Chrome Metal Powder for 3D Laser printer for Dental Metal Coping and Bridge
Powder Particle Size : D10 ≥ 10 μm , D50 30 ± 10 μm , D90 ≤ 45 μm
Proof Stress (Rp) : ≥ 500 Mpa
Metal Ceramic Bouding Properties : > 25 Mpa
Vikers Hardness : 450 ± 45 HV 10
CTE : 14.5 ± 0.5 * 10¯6 K¯1
Elongation : 2-10%