Product Description
DLX FeCrAl 0Cr25Al5 iron chromium aluminium Electric heating electric stove wire
1. Introduction to products
FeCrAl alloy is a ferritic iron-chromium-aluminium alloy with high resistivity and has superior oxidation resistance for use at temperatures up to 1450 centigrade degree., as compared to other commercial Fe and Ni base alloy.
2. Application
Our Products are widely applied to chemical industry, metallurgy mechanism, glass industry, ceramic industry, home appliance area and so on.
The wire used in an electric heating electric stove is typically made of a heat-resistant material, such as nickel-chromium alloy or iron-chromium-aluminum alloy. These alloys have high electrical resistance and can withstand the high temperatures generated by the stove. The wire is coiled or wound into a heating element, which is then connected to a power source to generate heat.
Alloy Nomenclature Performance | 1Cr13AL4 | 0Cr25Al5 | 0Cr21AL6 | 0Cr23Al5 | 0Cr21Al4 | 0Cr21Al6Nb | 0Cr27Al7Mo2 |
Main Chemical composition | Cr | 12.0-15.0 | 23.0-26.0 | 19.0-22.0 | 20.5-23.5 | 18.0-21.0 | 21.0-23.0 | 26.5-27.8 |
Al | 4.0-6.0 | 4.5-6.5 | 5.0-7.0 | 4.2-5.3 | 3.0-4.2 | 5.0-7.0 | 6.0-7.0 |
Re | opportune | opportune | opportune | opportune | opportune | opportune | opportune |
Fe | Rest | Rest | Rest | Rest | Rest | Rest | Rest |
| | | | | | Nb0.5 | Mo1.8-2.2 |
Max. continuous service temp. of element(°C) | 950 | 1250 | 1250 | 1250 | 1100 | 1350 | 1400 |
Resistivity at 20ºC(μΩ·m) | 1.25 | 1.42 | 1.42 | 1.35 | 1.23 | 1.45 | 1.53 |
Density(g/cm3) | 7.4 | 7.1 | 7.16 | 7.25 | 7.35 | 7.1 | 7.1 |
Thermal conductivity(KJ/m·h·ºC) | 52.7 | 46.1 | 63.2 | 60.2 | 46.9 | 46.1 | -- |
Coefficient of lines expansion(α×10-6/ºC) | 15.4 | 16 | 14.7 | 15 | 13.5 | 16 | 16 |
Melting point approx.( ºC) | 1450 | 1500 | 1500 | 1500 | 1500 | 1510 | 1520 |
Tensile strength(N/mm2) | 580-680 | 630-780 | 630-780 | 630-780 | 600-700 | 650-800 | 680-830 |
Elongation at rupture(%) | >16 | >12 | >12 | >12 | >12 | >12 | >10 |
Variation of area(%) | 65-75 | 60-75 | 65-75 | 65-75 | 65-75 | 65-75 | 65-75 |
Repeat Bending frequency(F/R) | >5 | >5 | >5 | >5 | >5 | >5 | >5 |
Hardness(H.B.) | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 | 200-260 |
continuous service time(Hours/ ºC) | -- | ≥80/1300 | ≥80/1300 | ≥80/1300 | ≥80/1250 | ≥50/1350 | ≥50/1350 |
Micrographic structure | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite | Ferrite |
Magnetic properties | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic | Magnetic |