Modeling paste
Model: LH-tool®5200A/B
Material | 5200A | 5200B | Mixed |
Description | epoxy resin | curing agent | |
mixing ration | 1 | 1 | |
Color: | brown | white | brown |
mixed time:500g,25°(min) | 30 | ||
curing time before machining(20-25mm) (hours) | 6-8 | ||
layer thickness (mm) | max.40 | ||
Density:(g/cm³): | 0.7-0.8 | ||
Hardness(Shore D): | 65-70 | ||
Temperature Resistance(°C): | 70-75 | ||
Coefficient of Thermal Expansion(10-6 K-1): | 45-50 | ||
Compressive Strength(N/mm²): | 16.2 | ||
Flexural Strength(N/mm²): | 19.2 | ||
Tensile Strength(N/mm²): | 12.4 | ||
Package(kg) | 10 | 10 |
Characteristics:
easily shaped and machined,fine surface structure
Applications:
yacht model,benchmark model, system and sand-cast model, rapid prototype,etc.