Silicon steel used in lamination mainly reducesHysteresis loss,Eddy current losses,Copper loss. In order to minimize the eddy currents more,magnetic core is laminated . The hysteresis coefficient of silicon steel is less, so hysteresis loss can be reduced.
Introduction:
Single phase UI core is made by the silicon steel strip. The model of UI lamination in standard sizes is from
UI 20-UI 100.The gap sizes of transformer lamination core can be customized.
SIZE | UI20---UI 100 |
THCIKNESS | 0.23-0.35MM (CRGO) 0.35-0.5MM (CRNGO) |
MATERIAL | M3, M4, M5, M6 (CRGO) 35W250, 35W300, 35W400 (0.35MM) 50W250, 50W310, 50W400, 50W470, 50W600, 50W800 (0.5MM) |
FREQUENCY | 50HZ-60HZ |
COATING | T2 Inorganic ( CRGO ) T4 Semi-organic (CRNGO) |
PROCESS TECHNOLOGY | ANNEALLING & WITHOUT ANNEALLING |
APPLICATION | CONTROL TRANSFORMER, AUTO TRANSFORMER, ISOLATION TRANSFORMER, POWER TRANSFORMER; BALLAST, REACTOR,INDUCTOR,INVERTER POWER, VOLTAGE STABILIZERS.etc |
Catalogue:
Type | a | b | c | d | e | holes | aperture(Φ) |
UI-20 | 60 | 20 | 20 | 60 | 4 | 6 | |
UI-22 | 66 | 22 | 22 | 66 | 4 | 6,8 | |
UI-25 | 75 | 25 | 25 | 75 | 4 | 6,8 | |
UI-27 | 81 | 27 | 27 | 81 | 4 | 6,8 | |
UI-28 | 84 | 28 | 28 | 84 | 4 | 8 | |
UI-30 | 90 | 30 | 30 | 90 | 4 | 8 | |
UI-32 | 96 | 32 | 32 | 96 | 4 | 8 | |
UI-35 | 105 | 35 | 35 | 105 | 4 | 8 | |
UI-38 | 114 | 38 | 38 | 114 | 4 | 8 | |
UI-40 | 120 | 40 | 40 | 120 | 4 | 10 | |
UI-44 | 132 | 44 | 44 | 132 | 4 | 8,10 | |
UI-45 | 135 | 45 | 45 | 135 | 4 | 10 | |
UI-50 | 150 | 50 | 50 | 150 | 4 | 8,10 | |
UI-60 | 180 | 60 | 60 | 180 | 4 | 10,12 | |
UI-70 | 210 | 70 | 70 | 210 | 4 | 13 | |
UI-80 | 240 | 80 | 80 | 240 | 4 | 14 | |
UI-90 | 270 | 90 | 90 | 270 | 4 | 14 | |
UI-100 | 300 | 100 | 100 | 300 | 4 | 16 |