Constant Elastic Alloy 0.125mmx25mm 3J53 Strip for Spring
Description:
Constant elastic alloy 3J53 is mainly for producing frequency components,such as precision sensors,precision spring,mechanical filter vibrators,turning forks for frequency resonances,reeds and films in resonance relays.
For 3J53(Ni42CrTi), the equivalent in other country is Ni-span C-902,Ni-Span C, Sumispan-3,42HXTIO,AMS 5225,UNS N09902,
Features:
Constant elastic alloys are characterized by a low frequency-temperature coefficient and good mechanical behavior under -40℃~+80℃.(Refer to our standard YB/T 5256-1993,YB/T 5254-1993)
Chemical content %:
Alloy | C | P | S | Si | Mn | Ni | Cr | Mo | Ti | Al | Fe |
Max | |||||||||||
3J53 | 0.05 | 0.02 | 0.02 | 0.8 | 0.8 | 41.5-43.5 | 5.2-5.8 | / | 2.3-2.7 | 0.5-0.8 | Bal. |
Physical Properties at Aging and Heat Treatment:
Alloy | Frequency temperature coefficient Bf(x10-6/℃) -40℃~+80℃ | Longtitudinal vibration wave transfer speed V(x10-6/℃) |
3J53 | A:0~20 B:0~10 | 4.80~5.05 |
Physical Properties at Cold Working and Aging Treatment:
Alloy | Dencity (g/cm3) | Average Coefficient Of Linear Expansion α20~100℃(x10-6/K) | Saturation Magnetic Induction B600(T) | Saturated Magnetostrictive Coefficient λs(x10-6) | Curie Temperature (℃) | Resistivity ρ(μΩ.m) |
3J53 | 8.0 | 8.1 | 0.7 | +5 | 110 | 1.1 |
Mechanical Properties at Cold Working and Aging Treatment:
Alloy | Elastic Modulus E(Mpa) | Shear Modulus G(Mpa) | Tensile Strength (Mpa) | Elongation (%) | Vickers Hardness (HV) |
3J53 | 176500~19100 | 63500~73500 | 1450 | ≥6 | 420 |
3J35 Application:
Tuning forks & Vibrating reeds
Leaf springs
Helical springs
Precision elastic parts
Diaphragms
Testing Equipment