Textured Geomembrane | ||||||||||||||
Item | Index | |||||||||||||
The thickness(mm) | 0.75 | 1.00 | 1.25 | 1.50 | 2.00 | 2.50 | 3.00 | |||||||
The density(g/cm3) | ≧0.94 | |||||||||||||
Roughness height (mm) | ≧0.25 | |||||||||||||
Tensile yield strength (longitudinal and transverse)N/mm | ≧11 | ≧15 | ≧18 | ≧22 | ≧29 | ≧37 | ≧44 | |||||||
Tensile fracture strength (longitudinal and transverse)N/mm | ≧8 | ≧10 | ≧13 | ≧16 | ≧21 | ≧26 | ≧32 | |||||||
Yield elongation (longitudinal and transverse)% | ≧12 | |||||||||||||
Elongation at break (longitudinal and transverse)% | ≧100 | |||||||||||||
Right-angle tearing load (longitudinal and transverse)N | ≧93 | ≧125 | ≧160 | ≧190 | ≧250 | ≧315 | ≧375 | |||||||
Puncture resistance N | ≧200 | ≧270 | ≧335 | ≧400 | ≧535 | ≧670 | ≧800 | |||||||
Stress cracking under tensile load (dead-load tensile method with notch)h | ≧300 | |||||||||||||
Carbon black content% | 2.0~3.0 | |||||||||||||
Oxidation induction time(OIT) min | Induction time of oxidation at atmospheric pressure≧100 | |||||||||||||
Induction time of high pressure oxidation≧400 | ||||||||||||||
85℃ thermal aging (OIT retention rate at atmospheric pressure after 90 days) % | ≧55 | |||||||||||||
Uv resistance (OIT retention rate after 1600h UV irradiation) % | ≧50 |
item | value |
Type | Geomembranes |
Warranty | More than 5 years |
After-sale Service | Return and Replacement |
Project Solution Capability | Others |
Application | Outdoor |
Place of Origin | China |
Shandong | |
Brand Name | LuXin |
Model Number | GH-2T |
Application | Landfill |
Color | Black White |
Material | HDPE EVA |
Product Name | Textured geomembrane |
Keyword | HDPE Geomembrane Waterproof |
Thickness | 0.2mm-2.8mm |
Surface | Double Texture Single Texture |
Length | 50m-100m/roll (as Request) |
Width | 1-6m |
Standard | ISO9001 |