ASTM B729 UNS N08020 Alloy 20 seamless nickel alloy pipe and tube
ASTM B468 /ASME SB468 Standard Specification for Welded UNS N08020 Alloy Tubes
| UNS N08020 | N08024 | N08026 | ||
ASTM B729 /ASME SB729 Specification for Seamless UNS N08020, UNS N08026, and UNS N08024 Nickel-Alloy Pipe and Tube
| UNS N08020 | UNS N08026 | UNS N08024 | ||
ASME SB474 /ASTM B474 Standard Specification for Electric Fusion Welded Nickel and Nickel Alloy Pipe
| UNS N02200 | UNS N02201 | UNS N04400 | UNS N06002 | UNS N06022 |
UNS N08825 | UNS N10276 | UNS N10665 | UNS N10675 | UNS N08026 | |
UNS N06030 | UNS N06200 | UNS N06230 | UNS N06600 | UNS N06601 | |
UNS N06625 | UNS N06985 | UNS N08020 | |||
ASTM B464 /ASME SB464 Standard Specification for Welded UNS N08020 Alloy Tubes
| UNS N08020 | N08024 | N08026 |
STANDARD | UNS | WNR. | AFNOR | EN |
Alloy 20 | N08020 | 2.4660 | Z2NCUD31-20AZ | NiCr20CuMo |
Grade | Ni | C | Mn | P | S | Si | Cr | Nb | Mo | Cu |
Alloy 20 | 32 - 38 | 0.02 max | 1 - 2 | 0.02 max | 0.005 max | 0.7 max | 19 - 21 | 0.1 - 0.3 | 2 - 3 | 3 - 4 |
Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
Alloy 20 | 8.1 g/cm3 | 1443 °C (2430 °F) | Psi -80,000, MPa -551 | Psi - 35,000, MPa - 241 | 30 % |
3. Common Test For Alloy 20 pipe we do:
4. Alloy 20 pipe and tube process technics: