STANDARD | UNS | WNR. |
Hastelloy C2000 | N06200 | 2.4675 |
Grade | Ni | Mo | Cr | Fe | W | Co | Mn | C | V | P | Si |
Hastelloy C2000 | Remainder | 15.0-17.0 | 14.5-16.5 | 4.0-7.0 | 3.0-4.5 | 2.5 max | 1.0 max | .01 max | .35 max | .04 max | .08 max |
Grade | Tensile Strength | Yield Strength | Elongation at break |
Hastelloy C2000 | 690 MPa | 310 MPa | 45% |
Surface | Black,bright,rough turned,grinding,centreless Ground etc |
Standard | GB,AISI,ASTM,DIN,EN,SUS,UNS etc |
Diameter | 0.5-500mm |
Technique | Hot Rolled,Cold Rolled,Cold Drawn,Forged |
Grade | Alloy : Alloy 20/28/31; Hastelloy: Hastelloy B / B-2/B-3/C22/C-4/S/ C276/C-2000/G-35/G-30/X/N; Haynes: Haynes 230/556/188; Inconel: Inconel 100/600/601/602CA/617/625713/718738/X-750,Carpenter 20; Incoloy: Incoloy 800/800H/800HT/825/925/926; GH: GH2132,GH3030,GH3039,GH3128,GH4180,GH3044 Monel: Monel 400/K500 Nitronic: Nitronic 40/50/60; Nimonic: Nimonic 75/80A/90 ; Nickle: Nickle 200/201; |
Alloy (UNS) | Ni | Cr | Mo | W | Cu | Fe | Carbon |
C276 (N10276) | Bal | 14.50-16.50 | 15.00-17.00 | 3.00-4.50 | – | 4.00-7.00 | 0.010max. |
22 (N06022) | Bal | 20.00-22.50 | 12.50-14.50 | 2.50-3.50 | – | 2.00-6.00 | 0.015max. |
59 (N06059) | Bal | 22.00-24.00 | 15.00-16.50 | – | – | 1.00 nom. | 0.010max. |
686 (N06686) | Bal | 19.00-23.00 | 15.00-17.00 | 3.00-4.40 | – | 1.00 max. | 0.010max. |
C2000® (N06200) | Bal | 22.00-24.00 | 15.00-17.00 | – | 1.30-1.90 | 3.00 max. | 0.010max. |
Alloy | PREN INDEX | PRE INDEX |
686 | 51 | 74 |
59 | 47 | 76 |
C2000® | 47 | 76 |
22 | 46 | 65 |
C276 | 45 | 59 |