SHT800-SHY Hdpe Pipe Plastic Butt Fusion Welding Machine with heating plate
Close the two pipe ends and check the alignment of both ends. The misalignment at both ends of the pipe should not exceed 10% of the wall thickness.The part outside the frame of the pipe shall be supported by supports to reduce friction, and then be fastened with slips.
Butt Fushion Welding Machine Technical data:
SHT800 -SHY | Working Range | |
Caliber (mm) | 630, 710, 800 | |
Heating board max temp. | 270 °C | |
Temperature bias | “+/-5° | |
Pressure adjustment range | 0-10Mpa | |
Heating plate power | 12.5 Kw | |
Power of Heating plate: | 2.2 Kw | |
Hydraulic unit power | 1.5 Kw | |
Total power | 16.2 Kw | |
G.W./N.W.: | 1200 Kgs | |
Packing size: | 190*136*140cm | |
110*72*162cm | ||
79*56*51cm |
Welding procedure
1. Check whether the specification and pressure grade of the pipe to be welded are correct, and check whether there are bumps, bumps and scratches on the surface. If the depth of the scar exceeds 10% of the wall thickness of the pipe, it should be partially removed before use;
2. Clean the oil or foreign matters at both ends of the pipe with a clean cloth;
3. Place the pipe to be welded in the frame slip, so that the length of both ends is equal (as short as possible without affecting the milling and heating). The part outside the frame of the pipe shall be supported by supports to reduce friction, and then be fastened with slips;
4. Put in the milling cutter, first turn on the power switch of the milling cutter, then close both ends of the pipe and apply appropriate pressure until there are continuous chips at both ends, remove the pressure, wait for a moment, then withdraw the movable frame, turn off the power supply of the milling cutter and take out the milling cutter. The chip thickness should be about 0.2-0.5mm. The chip thickness can be adjusted by adjusting the height of the milling insert;
5. Close the two pipe ends and check the alignment of both ends. The misalignment at both ends of the pipe should not exceed 10% of the wall thickness, which can be improved by adjusting the straightness and the elastic slip of the pipe; the gap between the two ends of the pipe should not exceed 10% of the wall thickness, otherwise it should be milled again until the above requirements are met;
6. Clean the dust and residue on the surface of the heating plate (pay special attention not to scratch the nonstick layer on the surface of the heating plate);
7. After the temperature of the heating plate reaches the set value, put it into the rack and apply the specified pressure until the minimum crimping on both sides reaches the specified value;
8. Reduce the pressure to the contact pressure and continue heating for the specified time;
9. When the time is up, withdraw the movable frame, quickly take out the heating plate, and then close the two pipe ends, with the time interval as short as possible;
10. Raise the pressure to the specified welding pressure, lock the fixing bolts on both sides of the frame, and keep the pressure for natural cooling. After cooling for the specified time, the fixing bolt is fully opened. Loosen the slip and take out the connected pipe.
Our service:
1) We offer 1 year warranty and free spare parts. (Except for wearing parts)
2) We offer voltage and frequency of motor customization service, such as 110v 60hz.