TZM alloy is Titnaium-Zirconium-Molybdenum Alloy and it is one of commonly used high temperature molybdenum alloy.
TZM alloy has good mechanical properties, especially at high temperature.
Physical performance comparison between TZM alloy and Pure Molybdenum
Material | Density (g/cm3) | Melting Point(℃) | boiling point(℃) |
TZM (Ti0.5/Zr0.1) | 10.22 | 2617 | 4612 |
Mo | 10.29 | 2610 | 5560 |
Mechanical property (TZM) | Elongation(%) | Elastic modulus(GPa) | Yield Strength (Mpa) | Tensile Strength(Mpa) | Fracture toughness(MP·m1/2) |
Value | <20 | 320 | 560~1150 | 685 | 5.8~29.6 |
TZM (Ti0.5/Zr0.08) High temperature tensile strength and elongation
Temperature/℃ | Properties | |
Tensile Strength/MPa | Elongation/% | |
RT | 1140 ~1210 | 7.5~13.0 |
1000 | 700 ~720 | 5.2 |
1200 | 320 ~360 | 9.0 |
1300 | 190 ~210 | 11.5 ~13.5 |
1400 | 140 ~170 | 11.0 ~16.0 |
TZM (Ti0.5/Zr0.1)Thermal and electrical properties
Properties | Coefficient of thermal expansion/K-1 (20~100℃) | Thermal conductivity W/m·K | Maximum temperature in air ℃ | Resistivity Ω·m |
Value | 5.3X10-6 | 126 | 400 | (5.3~5.5)X10-8 |
TZM alloy (molybdenum zirconium titanium alloy) also has good welding performance and can be well welded with H11 steel and other materials. At the same time, TZM alloy can resist the corrosion of liquid metal such as Zn. It can be cold worked by conventional methods. In the case of cooling lubricating oil, can use emented carbide or high-speed steel tools to machine.
Parameters
Thickness (mm) | Width (mm) | Length (mm) |
≥0.02 | 150 | L |
0.10-0.15 | 300 | 1000 |
0.15-0.20 | 400 | 1000 |
0.20-0.30 | 650 | 2540 |
0.30-0.50 | 650 | 2540 |
0.50-1.0 | 650 | 2540 |
1.0 -2.0 | 600 | 2000 |
2.0 -3.0 | 600 | 2000 |
> 3.0 | 600 | L |
TZM Molybdenum Alloy Applications
TZM molybdenum alloy can be applied for jet tube of flying vehicle and a variety of components of high temperature, high pressure turbine engine, such as hot gas seals and valves, turbine wheels or wheel blades.