Sintered Industrial Cylinder SmCo Rare Earth Magnet Zn Coating High Temp Resist
Product Paramenters
磁性能 | ||||||||||||||||||||
烧结钐钴磁体性能表(Magnetic Properties of Sintered SmCo Magnets) | ||||||||||||||||||||
牌号 | 剩磁 | 矫顽力 | 内禀矫顽力 | 最大磁能积 | 温度系数 | 最大工作温度Max.oper. Temp | 密度Density | |||||||||||||
Grade | Remanece ( 20°C) | Coercivity (20°C) | Intrinsic coercive force ( 20°C ) | Energy Density | Temp.coefficient %/C | |||||||||||||||
Br | Hcb | Hcj | (BH) max | 20-100°C | 20-150°C | |||||||||||||||
Typ. | min | Min | Min | Typ. | min | Tk (Br) typ. | Tk (Hcj) typ. | Tk (Br) typ. | Tk (Hcj) typ | |||||||||||
KGs | Tesla | KGs | Tesla | KOe | KA/m | KOe | KA/m | MGOe | KJ/m3 | MGOe | KJ/m3 | %/°C | %/°C | %/°C | %/°C | °C | °F | g/cm3 | ||
SmCo5 | HSMAG/XG16 | 8.50 | 0.85 | 8.00 | 0.80 | 7.50 | 597 | 18.00 | 1433 | 16.00 | 127 | 14.00 | 111 | -0.04 | -0.14 | -0.045 | -0.22 | 250 | 482 | 8.1-8.3 |
HSMAG/XG18 | 9.00 | 0.90 | 8.50 | 0.85 | 8.00 | 664 | 18.00 | 1433 | 18.00 | 143 | 16.00 | 127 | -0.04 | -0.14 | -0.045 | -0.22 | 250 | 482 | 8.1-8.3 | |
HSMAG/XG20 | 9.50 | 0.95 | 8.80 | 0.88 | 8.50 | 677 | 15.00 | 1195 | 20.00 | 159 | 18.00 | 143 | -0.04 | -0.14 | -0.045 | -0.22 | 250 | 482 | 8.1-8.3 | |
Sm2Co17 | HSMAG/XG24A | 10.30 | 1.03 | 9.50 | 0.95 | 8.50 | 677 | 25.00 | 1990 | 24.00 | 191 | 22.00 | 175 | -0.03 | -0.18 | -0.035 | -0.19 | 350 | 662 | 8.3-8.5 |
HSMAG/XG26A | 10.50 | 1.05 | 10.30 | 1.03 | 9.00 | 716 | 25.00 | 1990 | 26.00 | 207 | 24.00 | 191 | -0.03 | -0.18 | -0.035 | -0.19 | 350 | 662 | 8.3-8.5 | |
HSMAG/XG28A | 10.70 | 1.07 | 10.50 | 1.05 | 9.50 | 756 | 20.00 | 1592 | 28.00 | 223 | 26.00 | 207 | -0.03 | -0.18 | -0.035 | -0.19 | 350 | 662 | 8.3-8.5 | |
HSMAG/XG30A | 11.00 | 1.10 | 10.70 | 1.07 | 10.00 | 796 | 20.00 | 1592 | 29.00 | 231 | 27.00 | 215 | -0.03 | -0.18 | -0.035 | -0.19 | 350 | 662 | 8.3-8.5 | |
HSMAG/XG30EH | 11.20 | 1.12 | 10.80 | 1.08 | 10.20 | 812 | 20.00 | 1592 | 29.50 | 235 | 28.00 | 223 | -0.03 | -0.18 | -0.035 | -0.19 | 350 | 662 | 8.3-8.5 | |
HSMAG/XG32A | 11.50 | 1.15 | 10.90 | 1.09 | 10.30 | 820 | 20.00 | 1592 | 30.50 | 243 | 28.50 | 226 | -0.03 | -0.18 | -0.035 | -0.19 | 350 | 662 | 8.3-8.5 | |
HSMAG/XG33EH | 11.70 | 1.17 | 11.00 | 1.10 | 10.50 | 836 | 20.00 | 1592 | 31.50 | 251 | 29.00 | 235 | -0.03 | -0.18 | -0.035 | -0.19 | 350 | 662 | 8.3-8.5 | |
HSMAG/XG18AH | 10.00 | 1.00 | 8.50 | 0.85 | 8.00 | 637 | 30.00 | 2388 | 18.00 | 143 | 15.00 | 119 | -0.02 | -0.15 | -0.03 | -0.16 | 400 | 752 | 8.3-8.5 | |
Note | For large bread products, no thin size is allowed, because SmCo's huge brittleness will easily cause breakage during assembly |
Application
1). Electronics – Sensors, hard disk drives, sophisticated switches, electro-mechanical devices etc.;
2). Auto Industry – DC motors (hybrid and electric), small high-performance motors, power steering;
3). Medical – MRI equipment and scanners;
4). Clean Tech Energy – Water flow enhancement, wind turbines;
5). Magnetic Separators – Used for recycling, food and liquids QC, waste removal;
6). Magnetic Bearing – Used for highly sensitive and delicate procedures in various heavy industries.
The components of Samarium and Cobalt?
SmCo5 magnet is composed of SmCo alloy with Sm Co ratio of 1:5. According to weight, Sm accounts for 36% of the total. This SmCo alloy usually contains 36% Sm and a small amount of Co. This series of SmCo magnets can provide a maximum magnetic energy product of 25 MGOe and a reversible temperature coefficient of - 0.05% / ℃. In addition, this series is easier to calibrate to a specific magnetic field than Sm2Co17 series. The Sm2Co17 magnet consists of SmCo alloy with a SmCo ratio of 2:17. It also contains other elements, such as iron, copper, zirconium and hafnium in a small amount. The magnetic energy product of this property is higher, up to 32 MGOe, and the reversible temperature coefficient is - 0.03% / ℃.
The specific proportion is Sm: 23-28%; Rare earth metal Cobalt: 48-52%; Metallic element Fe: 14-17%; Metal element Cu: 5-7%; A small amount of Zr: 2-3 was added.
Sm | 23-28% |
Co | 48-52% |
Fe | 14-17% |
Cu | 5-7% |
Zr | 2-3% |
Our Certificate
Logistics And Trade