Magunion DC Motor Magnet Instrument and Meters -80~150℃ Working Temperature
Quick Details:
1. Application: Electric tool motor
2. Material grade: LT07,LT08, LT09
3. Shapes: arc, segments
4. Type: permanent ferrite magnet, sintered ferrite magnet
5. Material: ferrite, strontium, La2O3, CoO
Ferrite magnet (Ceramic magnet) is one of the most cost effective magnetic materials. Composed of Barium or Strontium ferrite, these materials exhibit good resistance to demagnetiztion, and are the lowest cost materials available today. It has a fair to good resistance toward corrosion and it can operate in moderate heat. Ceramic magnet has low energy product and they are usually used in assemblies containing mild steel. Sintered ferrite magnets are hard and brittle and are extensively used in cars, home appliances, fitness equipment, etc.
Applications:
DC motor
Speaker
MRI
Separators
Magnetron
Magnetor
Magnetic Door Catcher
Instrument and Meters
Toys
Arts and Crafts
Magunion Advantages:
Stable quality, good uniformity of performance and size
School-enterprise cooperation, provide professional customized motor magnet program.
Professional new production line, the delivery time of sample is on 7-10 days.
Merchandise name:
Ceramic magnet, permanent magnet, sintered magnet, powerful magnet, segment magnet, motor magnet, generator magnet, cylinder magnet, magnet material, magnetic product, permanent magnetic materials.
Physical Characteristics | ||||||||
Physical Properties | LT04 | LT05 | LT06 | LT07 | LT08 | LT09 | LT10 | LT11 |
Temperature Range (℃) | -40~+80 | -40~+80 | -40~+80 | -40~+80 | -40~+80 | -40~+80 | -40~+80 | -40~+80 |
Electrical Resistivity (Ω·m) | 104~108 | 104~108 | 104~108 | 104~108 | 104~108 | 104~108 | 104~108 | 104~108 |
Density (g/cm3) | 4.8~5.0 | 4.8~5.0 | 4.8~5.0 | 4.8~5.1 | 4.8~5.1 | 4.7~5.0 | 4.8~5.1 | 4.7~5.0 |
Recoil Permeability(rec) | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 | 1.05~1.03 |
Curie Temperature θt(℃) | 460 | 460 | 460 | 450~460 | 450~460 | 450~460 | 450~460 | 450~460 |
Temperature Coefficient of Remanence Br(%℃) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) | -(0.18~0.2) |
Linear Expansion Coefficient(10-6/℃) | 9~15 | 9~15 | 9~15 | 9~15 | 9~15 | 9~15 | 9~15 | 9~15 |
Magnet Properties | |||||||||
Type (Magunion) | Type (TDK) | Properties | |||||||
Br | Hcb | Hcj | BH(max) | ||||||
Gs | mT | Oe | kA/M | Oe | kA/M | MGOe | kJ/m3 | ||
LT01 | / | 3850±100 | 385±10 | >3100 | >246.8 | >3300 | >262.7 | 3.7±0.2 | 29.5±1.6 |
LT02 | FB5B | 4100±100 | 410±10 | 3200±150 | 242.4±11.9 | 3500±150 | 278.6±11.9 | 4.0±0.2 | 31.8±1.6 |
LT03 | / | 3950±100 | 395±10 | 3650±150 | 290.6±11.9 | 3900±150 | 310.5±11.9 | 3.8±0.2 | 30.2±1.6 |
LT04 | FB6B | 4200±100 | 420±10 | 3800±150 | 302.5±11.9 | 4000±150 | 318.4±11.9 | 4.2±0.2 | 33.5±1.6 |
LT05 | FB6H | 4000±100 | 400±10 | 3800±150 | 302.4±11.9 | 4500±150 | 358.1±11.9 | 3.7±0.2 | 29.4±1.6 |
LT06 | FB9B | 4500±100 | 450±10 | 4300±150 | 342.2±11.9 | 4500±250 | 358.2±11.9 | 4.9±0.2 | 38.4±1.6 |
LT07 | FBIH | 4300±100 | 430±10 | 4150±150 | 330.2±11.9 | 4800±250 | 382.1±11.9 | 4.4±0.2 | 35.0±1.6 |
LT08 | FB12H | 4600±100 | 460±10 | 4300±150 | 342±11.9 | 5000±250 | 398.1±11.9 | 5.2±0.2 | 41.4±1.6 |
LT09 | FB12B | 4700±100 | 470±10 | 4250±150 | 338.4±11.9 | 4700±250 | 374.2±11.9 | 5.4±0.2 | 43.1±1.6 |
LT10 | FB9N | 4600±100 | 460±10 | 3500±150 | 278.5±11.9 | 3600±150 | 286.5±11.9 | 5.1±0.2 | 40.4±1.6 |
LT11 | FB6N | 4400±100 | 440±10 | 3250±150 | 258.6±11.9 | 3300±150 | 262.7±11.9 | 4.5±0.2 | 35.9±1.6 |