Manufacture Supply Precision Alloy Invar 36 4J36 Sheet/Plate FeNi36
1 . Description
Invar 36, also known as FeNi36, is a nickel-iron, low-expansion alloy containing 36% nickel. It has a low coefficient of expansion from cryogenic temperatures to about 260°C. In the dry air at home temperature, invar 36 has good resistance to corrosion. But in moist air, it may go corrosion.
Invar 36 is suitable for the applications who require low coefficient of expansion, such as production, storage and transportation of liquid gas, temperature regulation devices working below 200°C, aperture mask, unit frameworks working below -200°C and so on.
Precision alloy series: 1J33,3J01,3J9,4J29,4J32.4J33,Invar36,4J45.FeNi50.
Main applications: Magnetic shunt compensatory element In the electromagnetic loop and the permanent magnetic loop.
2 . Chemical composition
Grade | C | Mn | S | P | Si | Cr | Ni | Fe |
Invar36 | ≤ 0.10 | ≤ 0.50 | ≤ 0.04 | ≤ 0.006 | ≤ 0.35 | 35-38% | rest |
3 . Tensile Strength (Strip & Sheet)
Termper Designation | Terper Name | Mpa |
A | Anealed | 586,Max |
B | 1/2 Hard | 593,Min |
C | Hard | 724,Min |