Material Grade :
UMCo50, cobalt alloy 1,cobalt alloy 3,
Working Temperature :
Up to 1200 Centi- degree
Hardness :
More than HRc50
Performance :
Better wear properrty and higher temperature
Cast Process :
Wax Lost Process
Description

Cobalts Alloy Castings Parts Nozzle with Wax Lost Process EB9064

Superalloy Castings Parts Cobalt Alloy Castings Parts Nozzle With Wax Lost Process

We produce High Temperature Superalloy Castings Parts with centrifugal cast process, investment process and resin sand cast process.
We melt good quality Co-based Alloy Castings with Vacuum Furnaces and Induction Furnaces.
We can cast and machine the hard Cobalt-based Alloy Castings as per the drawings.
We would like to help select suitable Co-based Alloy Grade as per your specific working condition.

Cobalt-based alloys have been in use for producing various components such as vanes or combustion chambers. The material can be implemented as wrought or as precision-cast parts or as centrifugal cast parts. The design of cobalt superalloys, which is aimed at an enhancement of both their oxidation resistance and their hot corrosion resistance, has received considerable impetus recently, especially since the advent of overlay coating techniques and the extensive studies which have been undertaken to elucidate the hot corrosion mechanisms and the effect of alloying elements.

Table 1 : Standard Cobalt & Nickel Base Alloys

cobalt alloy Alloy Overlay Welding

Co Cr C W Mo Ni Si B Fe Mn Others
cobalt alloy 1 BAL 33 2.45 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 3 BAL 31 2.5 13 - 2.5* 1 - 2.5* 1 -
cobalt alloy 4 BAL 31.5 1 14 - 2.0* 1 - 2.0* 1 -
BAL 28 1.2 5 - 3.0* 1 - 2.5* 1 -
cobalt alloy 12 BAL 29 1.85 9 - 2.5* 1 - 2.5* 1 -
cobalt alloy 20 BAL 33 2.45 17.5 - 2.5* 1 - 2.5* 1 -
cobalt alloy 21 BAL 27 0.25 - 5.5 2.5* 1 - 3.0* 1 -
cobalt alloy 31 BAL 26 0.5 7.5 - 10.5 1 - 2.0* 1 -
cobalt alloy 190 BAL 26 3.3 14 - 1.0 1 - 8.0 0.5 -
cobalt alloy 238 BAL 26 0.1 - 3 - 1 - 20.0 1 -
cobalt alloy 306 BAL 25 0.4 2 - 6.0 1 - 4.0* 1 Nb=5
94 BAL 28 1 19 - 5.0 1 - 2.5* 1 V=1
cobalt alloy F BAL 25.5 1.75 12.25 - 22.5 1 - 1.5* - -
cobalt alloy SF1 BAL 19 1.3 13 - 13 3 2.5 3* 0.5 Cu=0.5
cobalt alloy SF6 BAL 19 0.7 7 - 13 2.5 1.7 3* 0.5 Cu=0.5
cobalt alloy SF12 BAL 19 1 9 - 13 3 2 3* 0.5 Cu=0.5
cobalt alloy SF20 BAL 19 1.5 15 - 13 3 3 2* 0.5 Cu=0.5
TRIBALOY T400 BAL 8 0.1* - 28 3* 2.4 - 3* - -
TRIBALOY T800 BAL 17 0.1* - 28 3* 3.2 - 3* - -
DELORO 15 - - 0.06* - - BAL 2.0 1.05 1.5* 20 Cu=20
DELORO 22 - 0.70 0.10 - - BAL 2.3 1.75 - - -
DELORO 40 - 7.0 0.10 - - BAL 3.5 2.25 - - -
DELORO 50 - 10.25 0.45 - - BAL 4.0 1.85 4.0 - -
DELORO 60 - 14.25 0.6 - - BAL 2.0 3.5 4.0 - -
DELORO 625 - 22 0.1 - 9 BAL - - 5 - -
NISTELLE C - 16.5 0.12* 4.5 17 BAL 0.7 - 6.0 - -
TRIBALOY T700 - 15 0.10* - 32 BAL 3.25 -
Hastelloy C22®(UNS N06022)(Max.)
C MN P S Si Cr Ni Mo CO Fe W V
0.015 0.5 0.02 0.02 0.08 20.0-22.5 Bal. 12.5-14.5 2.5 2.0-6.0 2.5-3.5 0.35
Hastelloy C276®(UNS N10276)(Max.)
C MN P S Si Cr Ni Mo CO Fe W V
0.01 1 0.04 0.03 0.08 14.5-16.5 Bal. 15.0-17.0 2.5 4.0-7.0 3.0-4.5 0.35
Hastelloyx®(UNS N06002)(Max.)
C MN P S Si Cr Ni Mo CO Fe W other
0.05-0.15 1 0.04 0.03 1 20.5-23.0 Bal. 8.0-10.0 0.5-2.5 17.0-20.0 0.2-1.0 /
Monel 400®(UNS NO4400) (Max.)
C MN S Si Ni Cu Fe
0.3 2 0.024 0.5 63 min 28-34 2.5
Monel M400®(UNS NO4400)(Max.)
C MN S Si Ni Cu Fe
0.3 2 0.024 0.5 63-70 28-34 2.5
Monel R405®(UNS NO4405)(Max.)
C MN S Si Ni Cu Fe
0.3 2 0.025-0.06 0.5 63.0min 28-34 2.5
Monel K500®(UNS NO5500)(Max.)
C MN S Si Ni Cu Ti AI Fe
0.1 2 0.01 0.5 63min 27-33 0.86 2.3-3.15 2
Inconel 600(UNS NO6600)(Max.)
C MN S Si Cr Ni Cu Fe
0.15 1 0.015 0.5 14-17 72 min 0.5 6.0-10.0
Inconel 601(UNS NO6601)(Max.)
C MN Si Cr Ni CO AI Fe
0.05 0.3 0.2 22.5 61.5min 5 1.4 14.1
Inconel 718(UNS NO7718)(Max.)
Cr Ni Mo CO Cb+Ta Ti AI Fe
19 52.5min 3.05 5 5.13 0.9 0.5 18.5
Chemical Analysis of Incoloy 800® uns(N08800)
C Cr Ni Ti AI Fe Grain
0.1 max 19.0-23.0 30.0-35.0 0.15-0.6 0.15-0.6 39.5min /
Incoloy800H® UNS(N08810)
C Cr Ni Ti AI Fe Grain
0.05-0.1 19.0-23.0 30.0-35.0 0.15-0.60 0.15-0.60 39.5min 5or coarser
Incoloy800HT® UNS(N08811)
C Cr Ni Ti AI Fe Grain
0.06-0.10 19.0-23.0 30.0-35.0 0.25-0.60 0.25-0.60 39.5min 5or coarser

Production Process

Step 1: Getting orders.

Step 2: Process design by technical department

Step 3: Purchase of raw materials and pattern making &checking

Step 4: Inspection of raw materials

Step 5: Melting by middle-frequency induction furnaces

Step 6: Ladle analysis by Spectrometer

Step 7: De-oxidization, slag-removal, tapping

Step 8: Pouring

Step 9: Openning & fettling

Step 10: Surface & dimensional check

Step 11: Heat treatment

Step 12: Inspection of physical property (UT test,MT test, hardness,impact value µstructure)

Step 13: Packing

Step 14: Shipping

Send your message to this supplier
Send Now

Superalloy Castings Parts Cobalt Alloy Castings Parts Nozzle With Wax Lost Process

Ask Latest Price
Brand Name :
Eternal Bliss
Model Number :
EB9064
Certification :
ISO9001-2008
Place of Origin :
China
MOQ :
30kg
Price :
USD100~ USD150/kg
Contact Supplier
Superalloy Castings Parts Cobalt Alloy Castings Parts Nozzle With Wax Lost Process
Superalloy Castings Parts Cobalt Alloy Castings Parts Nozzle With Wax Lost Process
Superalloy Castings Parts Cobalt Alloy Castings Parts Nozzle With Wax Lost Process
Superalloy Castings Parts Cobalt Alloy Castings Parts Nozzle With Wax Lost Process
Superalloy Castings Parts Cobalt Alloy Castings Parts Nozzle With Wax Lost Process

Eternal Bliss Alloy Casting & Forging Co.,LTD.

Verified Supplier
8 Years
jiangsu, wuxi
Since 2013
Business Type :
Manufacturer, Distributor/Wholesaler, Agent, Importer, Exporter, Trading Company, Seller
Total Annual :
3,000,000-6,000,000
Certification Level :
Verified Supplier
Contact Supplier
Submit Requirement