99.95% Pure Vacuum Furnace Molybdenum Bar Polished Surface
Molybdenum (Mo) is a refractory metallic element that readily forms hard, stable carbides and has the sixth-highest melting point of any element. Molybdenum is most commonly used as a high-temperature, corrosion-resistant metal alloy in steel, cast iron, and supealloys for the military and defense industry, semiconductor industry and specialty machine shops.
Specification
Diameter |
0.125 (3.18 mm) 6 (152 mm) |
LengthVarious lengths are available |
|
Purity |
Mo≥99.95% |
Material |
Pure Molybdenum, Molybdenum TZM, Mo- La alloy |
Standard |
ASTM B-387 |
Properties
*If the diameter is <0.125”, please check our Molybdenum wire.
Molybdenum rod and molybdenum bar are formed by sintering molybdenum powder. Molybdenum rod has a high melting point, good thermal conductivity, and low thermal expansion performance. It can be used to manufacture electric vacuum devices and electric light source parts, and can also be used as high-temperature heating elements, high-temperature structural parts, electrodes, etc.
Please view the molybdenum rod to see our standard sizes of round bars. The above are most of the standard sizes of our molybdenum rectangular bars. If you do not see the size of the molybdenum bar you require, please contact us.
Molybdenum Rod Surface
Cleaned: The surface is chemically cleaned to remove all lubricants and oxides.
Black: The surface is either swaged or drawn and retains a coating of processing lubricants and oxides.
Chemical composition
Grade |
Molybdenum(Mo) (%) |
The impurity content is not more than (%) |
|||||||
Fe |
Ni |
Al |
Si |
Mg |
C |
N |
O |
||
Mo-1 |
99.95 |
0.01 |
0.005 |
0.002 |
0.01 |
0.005 |
0.01 |
0.003 |
0.008 |
Atomic number |
42 |
CAS number |
7439-98-7 |
Atomic mass |
95.94 [g/mol] |
Melting point |
2620 °C |
Boiling point |
4639 °C |
Density at 20 °C |
10.22 [g/cm] |
Crystal structure |
Body-centered cubic |
Coefficient of linear thermal expansion at 20 °C |
5.210-6[m/(mK)] |
Thermal conductivity at 20 °C |
142 [W/(mK)] |
Specific heat at 20 °C |
0.25 [J/(gK)] |
Electrical conductivity at 20 °C |
17.9106[S/m] |
Specific electrical resistance at 20 °C |
0.056 [(mm2)/m] |
Applications
Furnace pillars for sapphire crystal furnaces and other vacuum furnaces
Furnace heater for sapphire crystal furnaces and other vacuum furnaces
Tungsten headpieces for the industries of quartz