1. Product Name: ASTM A178 Electric Resistance Welded Carbon Steel and Manganese Steel Boiler and Superheater Tubes
2. Size Range: OD: 12.7-127mm, WT: 0.9-9.1mm, Length: 5.8m/6m, maximal 11.8m
3. Stable Quality with Comeptitive Price
4. High Preformance and Longer Working Life
Quality Control:
1. Incoming Raw Material Inspection
2. Raw Material Segregation to avoid steel grade mix-up
3. Heating and Hammering End for Cold Drawing
4. Cold Drawing or Cold Rolling, On line inspection
5. Heat Treatment
6. Straightening/Cutting to specified length/Finished Measuring Inspection
7. Quality Testing in own lab with Tensile Strength, Yield Strength, Elongation, Hardness, Straightness, etc.
8. Packing and Stocking.
100% Eddy Current Testing.
100% Size Tolerance Checking.
100% Tube surface checking to avoid surface defects.
Product Name | ASTM A178 Electric Resistance Welded Carbon Steel Boiler Tubes |
Material | Grade A, Grade C, Grade D |
Delivery Condition | Heat Treatment |
Standard | ASTM A179 |
Application | Heat Exchanger, Condensers and similar heat transfer apparatus |
Certificate | ISO 9001 |
HS code | 7304319000 |
Delivery Time | 40 days |
Packing | Bundles or Wooden Boxes |
Chemical Properties
Element | Grade A,Low-Cabon Steel | Grade C,Medium-Carbon Steel | Grade D, Carbon-Manganese Steel | |
Carbon | 0.06-0.18 | 0.35 Max | 0.27Max | |
Manganese | 0.27-0.63 | 0.80Max | 1.00-1.50 | |
Phosphorus,Max | 0.035 | 0.035 | 0.030 | |
Sulfur,Max | 0.035 | 0.035 | 0.015 | |
Silicon | - | - | 0.10 min | |
Mechanical Properties | Grade A | Grade C | Grade D | |
Tensile Strength:min ksi(Mpa) | 47(325) | 60(415) | 70(485) | |
Yield Point:min ksi(Mpa) | 26(180) | 37(255) | 40(275) | |
Elongation | ≥35% | ≥30% | ≥30% |