Manufacture:
The tubes are manufactured from hot or cold rolled plates, sheet or strips in accordance with EN10028-1,
longitudinally arc or laser welded by fusion accross the abutting edges
Manufacturing process
- Automatic arc welding
- Laser welding
Chemical Requirement | ||||||||
Grade: | … | TPXM-19 | TPXM-10 | TPXM-11 | TPXM-29 | TP304 | TP304L | TP304H |
UNS | S20400 | S20910 | S20900 | S21904 | S24000 | S30400 | S30403 | S30409 |
C, max | 0.03 | 0.060 | 0.080 | 0.04 | 0.08 | 0.08 | 0.035 | 0.040-0.10 |
Mn, max | 7.0-9.0 | 4.0-6.0 | 8.0-10.0 | 8.0-10.0 | 11.5-14.5 | 2.00 | 2.00 | 2.00 |
P, max | 0.045 | 0.045 | 0.045 | 0.045 | 0.060 | 0.045 | 0.045 | 0.045 |
S, max | 0.030 | 0.030 | 0.030 | 0.030 | 0.030 | 0.030 | 0.030 | 0.030 |
Si, max | 1.00 | 1.00 | 1.00 | 1.00 | 1.00 | 1.00 | 1.00 | 1.00 |
Cr | 15.0-17.0 | 20.5-23.5 | 19.0-21.5 | 19.0-21.5 | 17.0-19.0 | 18.0-20.0 | 18.0-20.0 | 18.0-20.0 |
Ni | 1.50-3.00 | 11.5-13.5 | 5.5-7.5 | 5.5-7.5 | 2.3-3.7 | 8.0-11.0 | 8.0-13.0 | 8.0-11.0 |
Mo | … | 1.50-3.00 | … | … | … | … | … | … |
Ti | … | … | … | … | … | … | … | … |
Columbium | … | 0.10-0.30 | … | … | … | … | … | … |
Tantalum | … | … | … | … | … | … | … | … |
Nitrogen | 0.15-0.30 | 0.20-0.40 | 0.15-0.40 | 0.15-0.40 | 0.20-0.40 | … | … | … |
Vanadium | … | 0.10-0.30 | … | … | … | … | … | … |
Copper | … | … | … | … | … | … | … | … |
Cerium | … | … | … | … | … | … | … | … |
Boron | … | … | … | … | … | … | … | … |
Aluminum | … | … | … | … | … | … | … | … |
Grade: | … | TP304N | TP304LN | … | … | … | TP309S | TP309H |
UNS | S30415 | S30451 | S30453 | S30600 | S30615 | S30815 | S30908 | S30909 |
C, max | 0.040-0.10 | 0.080 | 0.035 | 0.018 | 0.16-0.24 | 0.05-0.10 | 0.080 | 0.040-0.10 |
Mn, max | 0.80 | 2.00 | 2.00 | 2.00 | 2.00 | 0.80 | 2.00 | 2.00 |
P, max | 0.045 | 0.045 | 0.045 | 0.020 | 0.030 | 0.040 | 0.045 | 0.045 |
S, max | 0.030 | 0.030 | 0.030 | 0.020 | 0.030 | 0.030 | 0.030 | 0.030 |
Si, max | 1.00-2.00 | 1.00 | 1.00 | 3.7-4.3 | 3.2-4.0 | 1.40-2.00 | 1.00 | 1.00 |
Cr | 18.0-19.0 | 18.0-20.0 | 18.0-20.0 | 17.0-18.5 | 17.0-19.0 | 20.0-22.0 | 22.0-24.0 | 22.0-24.0 |
Ni | 9.0-10.0 | 8.0-18.0 | 8.0-12.0 | 14.0-15.5 | 13.5-16.0 | 10.0-12.0 | 12.0-15.0 | 12.0-15.0 |
Mo | … | … | … | 0.20 | … | … | 0.75 | … |
Ti | … | … | … | … | … | … | … | … |
Columbium | … | … | … | … | … | … | … | … |
Tantalum | … | … | … | … | … | … | … | … |
Nitrogen | 0.12-0.18 | 0.10-0.16 | 0.10-0.16 | … | … | 0.14-0.20 | … | … |
Vanadium | … | … | … | … | … | … | … | … |
Copper | … | … | … | 0.5 max | … | … | … | … |
Cerium | … | … | … | … | … | 0.03-0.08 | … | … |
Boron | … | … | … | … | … | … | … | … |
Aluminum | … | … | … | … | 0.80-1.50 | … | … | … |
Grade: | TP309Cb | TP309HCb | … | TP310S | TP310H | TP310Cb | TP310HCb | … |
UNS | S30940 | S30941 | S31002 | S31008 | S31009 | S31040 | S31041 | S31050 |
C, max | 0.080 | 0.040-0.10 | 0.015 | 0.080 | 0.040-0.10 | 0.080 | 0.040-0.10 | 0.025 |
Mn, max | 2.00 | 2.00 | 2.00 | 2.00 | 2.00 | 2.00 | 2.00 | 2.00 |
P, max | 0.045 | 0.045 | 0.020 | 0.045 | 0.045 | 0.045 | 0.045 | 0.020 |
S, max | 0.030 | 0.030 | 0.015 | 0.030 | 0.030 | 0.030 | 0.030 | 0.015 |
Si, max | 1.00 | 1.00 | 0.15 | 1.00 | 1.00 | 1.00 | 1.00 | 0.40 |
Cr | 22.0-24.0 | 22.0-24.0 | 19.0-22.0 | 24.0-26.0 | 24.0-26.0 | 24.0-26.0 | 24.0-26.0 | 24.0-26.0 |
Ni | 12.0-16.0 | 12.0-16.0 | 24.0-26.0 | 19.0-22.0 | 19.0-22.0 | 19.0-22.0 | 19.0-22.0 | 20.5.0-23.5 |
Mo | 0.75 | 0.75 | 0.10 | 0.75 | … | 0.75 | 0.75 | 1.6-2.6 |
Ti | … | … | … | … | … | … | … | … |
Columbium | 10XC min,1.10 max | 10XC min,1.10 max | … | … | … | 10XC min,1.10 max | 10XC min,1.10 max | … |
Tantalum | … | … | … | … | … | … | … | … |
Nitrogen | … | … | 0.10 | … | … | … | … | 0.09-0.15 |
Vanadium | … | … | … | … | … | … | … | … |
Copper | … | … | … | … | … | … | … | … |
Cerium | … | … | … | … | … | … | … | … |
Boron | … | … | … | … | … | … | … | … |
Aluminum | … | … | … | … | … | … | … | … |
1~ Incoming Raw Material Inspection
2~ Raw Material Segregation to avoid steel grade mix-up
3~ Heating and Hammering End for Cold Drawing
4~ Cold Drawing and Cold Rolling, on line inspection
5~ Heat Treatment, +A, +SRA, +LC, +N, Q+T
6~ Straightening-Cutting to specified length-Finished Measuring Inspection
7~ Machanical Testing in own labs with Tensile Strength, Yield Strength, Elongation, Hardness, Impact, Mictrostruture etc
8~ Packing and Stocking.
100% of our steel tubes are dimensionally checked
100% of our steel tubes are visually checked to assure they have a perfect surface condition and no surface defects.
100% eddy current test and ultrosonic test to eliminate longitudinal and transversal defects.
.