Application: For condensers and heat-exchangers
Technique: Cold Drawn and Hot-Finished
Size:
OD | 5-420mm |
WT | 1-50mm |
LENGTH | Max 12000mm |
Referenced Documents:
ASTM Referenced Standards
A370 Test methods and Definitions for mechanical testing of steel products.
E8 Test methods for tension testing of metallic materials.
E29 practice for using significant digits in test data to determine conformance with specifications.
E120 Test Methods for chemical analysis of titanium and titanium alloys.
E1409 Test method for determination of oxygen in titanium and titanium alloys by the inert gas fusion technique.
E1447 test method for determination of hydrogen in titanium and titanium alloys by the inert gas fusion thermal conductivity method.
Chemical Composition:
Element | Composition % | |||||
Grade 1 | Grade 2 | Grade 3 | Grade 7 | Grade 9 | Grade 11 | |
Nitrogen, max | 0.03 | 0.03 | 0.05 | 0.03 | 0.03 | 0.03 |
Carbon, max | 0.08 | 0.08 | 0.08 | 0.08 | 0.08 | 0.08 |
Hydrogen, max | 0.015 | 0.015 | 0.015 | 0.015 | 0.015 | 0.015 |
Iron, max | 0.2 | 0.3 | 0.3 | 0.3 | 0.25 | 0.25 |
Oxygen, max | 0.18 | 0.25 | 0.35 | 0.25 | 0.15 | 0.15 |
Aluminum | … | 2.5-3.5 | 2.5-3.5 | |||
Vanadium | … | 2.0-3.0 | 2.0-3.0 | |||
Tin | … | |||||
Ruthenium | … | |||||
Palladium | … | 0.12-0.25 | ||||
Cobalt | … | |||||
Molybdenum | … | |||||
Chromium | … | |||||
Nickel | … | |||||
Niobium | … | |||||
Zirconium | … | |||||
Silicon | … | |||||
Residuals, max each | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 | 0.1 |
Residuals, max total | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 | 0.4 |
Titanium | balance | balance | balance | balance | balance | balance |
Mechanical proporties:
Grade | Tensile strength, in | Yield Strength, 0.2% Offset | Elongation in 2 in. or 50mm, min, % | ||||
Ksi | Mpa | min | max | ||||
Ksi | Mpa | Ksi | Mpa | ||||
1 | 35 | 240 | 25 | 170 | 45 | 310 | 24 |
2 | 50 | 345 | 40 | 275 | 65 | 450 | 20 |
3 | 65 | 450 | 55 | 380 | 80 | 550 | 18 |
7 | 50 | 345 | 40 | 275 | 65 | 450 | 20 |
9 | 125 | 860 | 105 | 725 | … | … | 10 |
11 | 35 | 240 | 25 | 170 | 45 | 310 | 24 |
Tubing shall withstand, without cracking, flattening under a load applied gradually at room temperature until the distance between the load platens is not more than H in. H is calculated as SB338 standard.
For tube 3 1/2 in.(88mm) in outside diameter and smaller, and 0.134 in.(3.4mm) in wall thickness and thinner, a section of tube approximately 4 in.(102mm) in length shall withstand being flared with a tool having a 60°included angle until the tube at the mouth of the flare has been expanded in accordance with table4 the flared end shall show no cracking or rupture visible to the unaided eye. Flaring tests on larger diameter tube or tubing outside the range of standard shall be as agreed upon between the manufacturer and the purchaser.
Welded tubing shall be tested using both a nondestructive electromagnetic test and an ultrasonic test as described in standard. Seamless and welded/cold worked tubing shall be tested using an ultrasonic test as described in standard.
Welded or seamless tubing shall be tested with a hydrostatic or pneumatic test as described in standard. Other requirements details can check standard.
Product show:
Q: Are you trading company or manufacturer?
A: We are a professional steel pipes materials manufacturer.
Q: How long is your delivery time?
A: Generally it takes 7-14 days if the goods are in stock or 30-60 days if there is no stock, this mainly depends on quantity.
Q: Do you provide free samples?
A: Yes, we could offer the sample for free charge but need pay the cost of freight.
Q: What is your terms of payment?
A: Payment<=1000USD, 100% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shippment.
If you have another question, pls feel free to contact us.