Type 434 is one of the most widely used of the "non-hardenable" ferritic stainless steels. The addition of molybdenum increases this alloy's corrosion resistance and its attack to many deicing chemicals. It combines good heat and oxidation resistance up to 1500 °F (816 °C) as well as good mechanical properties.
434 ferritic Stainless Steel precision Strip Coil / Rolls Equivalent Materials
AISI 434 equivalents | ||
0 | DIN 1.4113 | |
1 | DIN X6CrMo17 | |
2 | DIN X6CrMo17-1 | |
3 | AFNOR Z8CD17-01 | |
4 | BS 434S17 | |
5 | UNI X8CrMo17 | |
6 | SS 2325 | |
7 | AISI S43400 | |
8 | SAE 434 | |
9 | SAE S43400 | |
10 | JIS SUS434 | |
11 | EN X6CrMo17-1 | |
12 | EN 1.4113 | |
13 | UNS S43400 |
439 Stainless Steel Strip Specifications
Grade: 439
Standard: ASTM/EN/JIS
Thickness: 0.03mm-3.0 mm
Width: 1.5mm-600 mm
Length: coil type or it can be produced as customer requirements
Surface Finish: NO.1, 2B, 2H(Rerolled Bright), BA, No.4, 8K (Mirror), HL (Hairline), Polishing Bright, etc
Edge: Mill Edge, Slit Edge, Deburred Edge, Round Edge, V Type Edge
Tempered Condition : | |
ANNEALED CONDITION | TEMPERED 1/16 HARD |
Tempered 1/8 Hard | TEMPERED 1/4 HARD |
TEMPERED 1/2 HARD | TEMPERED 3/4 HARD |
TEMPERED FULL HARD | Tempered Extra Hard |
Annealed | 2B /BA/ MIRROR / HL / SATIN / No.1 |
Architectural, automotive trim amd molding, furnace combustion chambers, dishwashers, range hoods, gas burners on heating units, gutters and down spouts, steam iron bases and flatware, nitric acid plant equipment, oil refinery equipment, roofing and siding and restaurant equipment
Carbon |
| 0.05 max |
Chromium |
|
|
Iron |
| Balance |
Manganese |
| 0.5 max |
Molybdenum |
|
|
Phosphorus |
| 0.03 max |
Silicon |
| 0.5 max |
Sulphur |
| 0.01 max |
| |
Density (lb / cu. in.) | 0.277 |
Specific Gravity | 7.65 |
Specific Heat (Btu/lb/Deg F - [32-212 Deg F]) | 0.11 |
Melting Point (Deg F) | 2750 |
Form |
| Strip | ||
Condition |
| Test Specimen Annealed | ||
Temper |
| 70 | ||
Tensile Strength |
| 74 | ||
Yield Strength |
| 49 | ||
Elongation |
| 26 | ||
| ||||
Form |
| Strip | ||
Condition |
| Test Specimen Annealed | ||
Temper |
| 200 | ||
Tensile Strength |
| 70 | ||
Yield Strength |
| 47 | ||
Elongation |
| 23 | ||
| ||||
Form |
| Strip | ||
Condition |
| Test Specimen Annealed | ||
Temper |
| 400 | ||
Tensile Strength |
| 68 | ||
Yield Strength |
| 42 | ||
Elongation |
| 18 | ||
| ||||
Form |
| Strip | ||
Condition |
| Test Specimen Annealed | ||
Temper |
| 600 | ||
Tensile Strength |
| 65 | ||
Yield Strength |
| 38 | ||
Elongation |
| 18 | ||
| ||||
Form |
| Strip | ||
Condition |
| Test Specimen Annealed | ||
Temper |
| 800 | ||
Tensile Strength |
| 62 | ||
Yield Strength |
| 34 | ||
Elongation |
| 17 | ||
| ||||
Form |
| Strip | ||
Condition |
| Test Specimen Annealed | ||
Temper |
| 1000 | ||
Tensile Strength |
| 45 | ||
Yield Strength |
| 25 | ||
Elongation |
| 26 | ||
| ||||
Form |
| Strip | ||
Condition |
| Test Specimen Annealed | ||
Temper |
| 1200 | ||
Tensile Strength |
| 18 | ||
Yield Strength |
| 13 | ||
Elongation |
| 69 | ||
| ||||
Form |
| Strip | ||
Condition |
| Test Specimen Annealed | ||
Temper |
| 1400 | ||
Tensile Strength |
| 6.5 | ||
Yield Strength |
| 4.9 | ||
Elongation |
| 86 | ||
| ||||
Form |
| Strip | ||
Condition |
| Test Specimen Annealed | ||
Temper |
| 1600 | ||
Tensile Strength |
| 4 | ||
Yield Strength |
| 2.8 | ||
Elongation |
| 79 |