Alloy powder good tolerance shock base valve density 6.6 g/cm3 without steam treatment
Specifications:
Density | 6.2-6.8 g/cm3 |
Hardness | HRB 45-65 |
Steam treatment | 2H high temp steam holding time |
Thickness of Fe3O4 | 0.004-0.005mm |
Description:
HRB45-65 Iron-Copper and Copper Steel Sintered Parts for car shock absorbers
Our company produces different kinds of sintered parts. These sintered part include pistons, foot valve,
rod guider, valve base and so on.
Dimension: D32.5XD6X11.5
Material: MPIF FC-0205
Density: Not less than 6.5g/cm3
Net weight is 30.36g
Die tooling design and making in house
Ultrasonic clearing and auto de-burring
This is a foot valve.
2 symmetrical holes design
No lack of material of valve line
No foreign material and dust on surface
Material Available and Chemical Composition:
P/M Copper and Copper Alloys
P/M Iron and Carbon Steel
Iron and Carbon Steel
Iron-Copper and Copper Steel
Iron-Nickel and Nickel Steel
Low Alloy Steel
Commix Low Alloy Steel
Sinter Hardened Steel
Diffusion Alloyed Steel
Copper Infiltrated Iron and steel
Applications:
Automotive Part
Motorcycle Part
Metal Powder Sintered Parts
Locomotive Parts
Machinery Parts
Tool Parts
Competitive Advantage:
1. High precision |
2. 100% quality with competitive price |
3. Good abrasion resistance |
4. High efficiency |
5. Save energy |
Picture show: