SCH40S SCH80S SCH160S Hastelloy C276 Pipe Tube Seamless Pipe in 6m Length EN 2.4819
Specifications | ASTM B 622 ASME SB 622 / ASTM B 619 ASME SB 619 |
Dimensions | ASME, ASTM, and API |
Size | 15″NB upto 150″NB IN |
Specialized in | Sizes in Large Diameter |
Schedule | Schedule 5, 10, 40, STD, 80, 160 |
Type | ERW / Seamless / Welded / LSAW Pipes / Fabricated |
Form | Hydraulic, Round, Etc |
Length | Double Random, Single Random, & Cut Length. |
End | Beveled End, Plain End, Treaded |
Hastelloy C276 Pipe Specification
Alloy C276 Seamless Pipe
WNR 2.4819 Welded Pipe
Nickel C276 Thick-Walled Pipe
International Specification
About Hastelloy C276 Pipe
Useful Information
Nickel alloy c276 cold finished pipe welded pipe services
WNR 2.4819 bright annealed pipe features
NW 0276 Cold Finished Seamless Pipe Marking
EN 2.4819 round pipe inspection checklist
UNS N10276 Annealed Pipe Documentation Offered
Nickel C276 Annealed Pipe Equipment
EN 2.4819 Pipe Welding Method
Alloy C276 Seam Welded Pipe Physical Properties
Alloy C276 Seamless Pipe Properties
C | W | Mn | Fe | S | Si | Cr | Ni | Co | Mo | P | V | |
---|---|---|---|---|---|---|---|---|---|---|---|---|
MIN | - | 3.000 | - | 4.000 | - | - | 14.500 | Bal | - | 15.000 | - | - |
MAX | 0.010 | 4.500 | 1.000 | 7.000 | 0.030 | 0.080 | 16.500 | 2.500 | 17.000 | 0.040 | 0.035 |
Yield Strength0.2% Proof(MPa) | Tensile strength(MPa) | Elongation (% in 50mm) | Hardness (HRB) | |
---|---|---|---|---|
MIN | 283 | 690 | 40.00 | - |
MAX | - | - | - | 100 |
Density | lb/in³ | 0.321 |
---|---|---|
g/cm³ | 8.89 | |
Specific Heat | Btu/lb•°F | 0.102 |
J/kg•°C | 427 | |
Melting Range | °F | 2415-2500 |
°C | 1325-1370 | |
Thermal Conductivity | Btu•in/ft²•h•°F | 67.9 |
W/m•°C | 427 | |
Young's Modulus | 103 ksi | 29.8 |
GPa | 205 | |
Shear Modulus | 103 ksi | 11.4 |
GPa | 79 | |
Permeability | 200 oersted (15.9 kA/m) | 1.0002 |
Poisson's Ratio | 0.307 |
Density | lb/in³ | 0.321 |
---|---|---|
g/cm³ | 8.89 | |
Specific Heat | Btu/lb•°F | 0.102 |
J/kg•°C | 427 | |
Melting Range | °F | 2415-2500 |
°C | 1325-1370 | |
Thermal Conductivity | Btu•in/ft²•h•°F | 67.9 |
W/m•°C | 427 | |
Young's Modulus | 103 ksi | 29.8 |
GPa | 205 | |
Shear Modulus | 103 ksi | 11.4 |
GPa | 79 | |
Permeability | 200 oersted (15.9 kA/m) | 1.0002 |
Poisson's Ratio | 0.307 |