ASTM A213 / ASME SA213 T11 Seamless Alloy Steel Tube Boiler Tube
ASTM A213 T11 tubes are primarily made from an alloy that includes chromium and molybdenum, which enhance the mechanical properties of the steel, including its strength and resistance to heat and corrosion. Specifically, T11 contains around 1% chromium and about 0.5% molybdenum, providing excellent high-temperature strength and oxidation resistance, making T11 a popular choice in industries such as power generation, petrochemical, and manufacturing.
Quality Control
Advantages: The primary advantages of using ASTM A213 T11 seamless tubes include:
SA213/A213 T11 Chrome Moly Alloy Steel Seamless Tube
Tube Sizes for Heat Exchangers & Condensers & Boiler | |||||||||
Outside Diameter | BWG | ||||||||
25 | 22 | 20 | 18 | 16 | 14 | 12 | 10 | ||
Wall Thickness mm | |||||||||
0.508 | 0.71 | 0.89 | 1.24 | 1.65 | 2.11 | 2.77 | 3.40 | ||
mm | inch | Weight kg/m | |||||||
6.35 | 1/4 | 0.081 | 0.109 | 0.133 | 0.174 | 0.212 | |||
9.53 | 3/8 | 0.126 | 0.157 | 0.193 | 0.257 | 0.356 | 0.429 | ||
12.7 | 1/2 | 0.214 | 0.263 | 0.356 | 0.457 | 0.612 | 0.754 | ||
15.88 | 5/8 | 0.271 | 0.334 | 0.455 | 0.588 | 0.796 | 0.995 | ||
19.05 | 3/4 | 0.327 | 0.405 | 0.553 | 0.729 | 0.895 | 1.236 | ||
25.4 | 1 | 0.44 | 0.546 | 0.75 | 0.981 | 1.234 | 1.574 | 2.05 | |
31.75 | 1 1/4 | 0.554 | 0.688 | 0.947 | 1.244 | 1.574 | 2.014 | 2.641 | |
38.1 | 1 1/2 | 0.667 | 0.832 | 1.144 | 1.514 | 1.904 | 2.454 | 3.233 | |
44.5 | 1 3/4 | 1.342 | 1.774 | 2.244 | 2.894 | 3.5 | |||
50.8 | 2 | 1.549 | 2.034 | 2.574 | 3.334 | 4.03 | |||
63.5 | 2 1/2 | 1.949 | 2.554 | 3.244 | 4.214 | 5.13 | |||
76.2 | 3 | 2.345 | 3.084 | 3.914 | 5.094 | 6.19 | |||
88.9 | 3 1/2 | 2.729 | 3.609 | 4.584 | 5.974 | 7.27 | |||
101.6 | 4 | 4.134 | 5.254 | 6.854 | 8.35 | ||||
114.3 | 4 1/2 | 4.654 | 5.924 | 7.734 | 9.43 |
ASTM A213/ASME SA213 T2, T11, T12, T22, T91, T92 Chemical Composition and Mechanical Properties
Grade | Chemical Composition% | ||||||||
C | Si | Mn | P, S Max | Cr | Mo | Ni Max | V | Al Max | |
T2 | 0.10~0.20 | 0.10~0.30 | 0.30~0.61 | 0.025 | 0.50~0.81 | 0.44~0.65 | – | – | – |
T11 | 0.05~0.15 | 0.50~1.00 | 0.30~0.60 | 0.025 | 1.00~1.50 | 0.44~0.65 | – | – | – |
T12 | 0.05~0.15 | Max 0.5 | 0.30~0.61 | 0.025 | 0.80~1.25 | 0.44~0.65 | – | – | – |
T22 | 0.05~0.15 | Max 0.5 | 0.30~0.60 | 0.025 | 1.90~2.60 | 0.87~1.13 | – | – | – |
T91 | 0.07~0.14 | 0.20~0.50 | 0.30~0.60 | 0.02 | 8.0~9.5 | 0.85~1.05 | 0.4 | 0.18~0.25 | 0.015 |
T92 | 0.07~0.13 | Max 0.5 | 0.30~0.60 | 0.02 | 8.5~9.5 | 0.30~0.60 | 0.4 | 0.15~0.25 | 0.015 |
Grade | Chemical Composition% | Mechanical Properties | |||||||
W | B | Nb | N | T. S | Y. P | Elongation | Hardness | ||
T2 | – | – | – | – | ≥ 415MPa | ≥ 205MPa | ≥ 30% | 163HBW(85HRB) | |
T11 | – | – | – | – | ≥ 415MPa | ≥ 205MPa | ≥ 30% | 163HBW(85HRB) | |
T12 | – | – | – | – | ≥ 415MPa | ≥ 220MPa | ≥ 30% | 163HBW(85HRB) | |
T22 | – | – | – | – | ≥ 415MPa | ≥ 205MPa | ≥ 30% | 163HBW(85HRB) | |
T91 | – | – | 0.06~0.10 | 0.03~0.07 | ≥ 585MPa | ≥ 415MPa | ≥ 20% | 250HBW(25HRB) | |
T92 | 1.50~2.00 | 0.001~0.006 | 0.04~0.09 | 0.03~0.07 | ≥ 620MPa | ≥ 440MPa | ≥ 20% | 250HBW(25HRB) |
Permissible variations from the specified minimum wall thickness shall be in accordance with Specification A1016/A1016M.
Outside Diameter | OD Tolerance | WT Tolerance | Ovality Tolerance | Cut Length Tolerance |
OD≤ 12, 7 mm | ± 0, 13 mm | ± 15 % | – | + 3, 18 mm, – 0 mm |
12, 7 mm < OD ≤ 38, 1 mm | ± 0, 13 mm | ± 10 % | max, 1, 65 mm | + 3, 18 mm, – 0 mm |
38, 1 mm < OD ≤ 88, 9 mm | ± 0, 25 mm | ± 10 % | max, 2, 41 mm | + 4, 76 mm, – 0 mm |
Applications