Alloy C276 is a nickel, chromium, and molybdenum alloy. The Hastelloy C276 is designed with excellent corrosion and oxidation resistance properties. HASTELLOY C-276 (Alloy C276, 2.4819, UNS N10276). HASTELLOY C276 (UNS N10276) is a nickel-chromium-molybdenum alloy with very high corrosion. Alloy C276 is one of the few materials resistant to wet chlorine gas, hypochlorite and chlorine dioxide.
Hastelloy C276 Specification
Check Hastelloy C276 Composition, Density, Hardness, Heat Treatment, and Price per kg in Mumbai, India
Standard | Hastelloy C276 |
---|
UNS | N10276 |
Werkstoff Nr. | 2.4819 |
Hastelloy Alloy C276 Chemical Equation
Hastelloy C276 | Analysis |
Ni | Bal |
Mo | 15 – 17 |
Cr | 14.5 – 16.5 |
Fe | 4 – 7 |
W | 3 – 4.5 |
Co | 2.5 max |
Mn | 1.0 max |
C | 0.01 max |
v | 0.35 max |
P | 0.04 max |
S | 0.03 max |
Si | 0.08 max |
Alloy C276 Mechanical Strength Table
Density | 8.89 g/cm3 |
Melting Point | 1370 °C (2500 °F) |
Tensile Strength | Psi – 1,15,000 , MPa – 790 |
Yield Strength (0.2%Offset) | Psi – 52,000 , MPa – 355 |
Elongation | 40 % |