These magnets are characterized by high magnetism, and are also resistant to both rust and high temperature.
These magnets represent the highest magnetic energy product after neodymium magnets. They are also highly
corrosion-resistant without being rustproofed and offer excellent temperature characteristics as well. These are
rare-earth magnets resistant to high temperature.
These sintered products consist mainly of samarium (Sm) and cobalt (Co), and are available with two kinds of material:
1-5 series and 2-17 series. The 1-5 series has high magnetic coercive force (Hcj), but is easy to magnetize and adjust
magnetism. Magnets of this series also exhibit relatively stable performance under changing temperature. The 2-17
series has high magnetism and offers excellent temperature stability in magnetic characteristics as well.
Samarium-cobalt magnets are relatively low in mechanical strength. Caution should therefore be exercised in handling
these magnets to prevent chipping and cracking.
Samarium Cobalt Magnets
Samarium cobalt magnets (SmCo) are composed of samarium, cobalt and iron. These rare earth magnets are extremely strong for their small size, metallic in appearance and found in simple shapes such as rings, blocks and discs.
Manufacturing - In general, the elements are melted together and milled into a powder that is dry-pressed
shape in the presence of a magnetic field. The material is then sintered, aged, ground to dimension, magnetized and tested. They are called “rare earth” magnets because the elements of samarium cobalt
classified as such in the lanthanides section of Periodic Table of the Elements.
Attributes of Samarium Cobalt
High resistance to demagnetization
High energy (magnetic strength is strong for its size)
Good temperature stability
Pricing for samarium cobalt is market sensitive
Grade | Remanence (Br) | Coercivity (Hcb) | Intrinsic Coercivity (Hcj) |
| Curie Temperature (TC) | Max Work Temp (TW) | Temperature Coefficient of Br (Br) | Temperature Coefficient of Hcj (Hcj) | |||||||
T | kGS | kA/m | KOe | KA/m | KOe | KJ/m3 | MGOe | ℃ | ℃ | %℃ | %℃ | ||||
YX-16s | 0.79-0.84 | 7.9-8.4 | 620-660 | 7.8-8.3 | ≥1830 | ≥23 | 118-135 | 15-17 | 750 | 250 | -0.035 | -0.28 | |||
YX-18s | 0.84-0.89 | 8.4-8.9 | 660-700 | 8.3-8.8 | ≥1830 | ≥23 | 135-151 | 17-19 | 750 | 250 | -0.040 | -0.28 | |||
YX-20s | 0.89-0.93 | 8.9-9.3 | 684-732 | 8.6-9.2 | ≥1830 | ≥23 | 150-167 | 19-21 | 750 | 250 | -0.045 | -0.28 | |||
YX-22s | 0.92-0.96 | 9.2-9.6 | 710-756 | 8.9-9.5 | ≥1830 | ≥23 | 167-183 | 21-23 | 750 | 250 | -0.045 | -0.28 | |||
YX-24s | 0.96-1.00 | 9.6-10.0 | 740-788 | 9.3-9.9 | ≥1830 | ≥23 | 183-199 | 23-25 | 750 | 250 | -0.045 | -0.28 | |||
LTc(YX-10) | 0.62-0.66 | 6.2-6.6 | 485-517 | 6.1-6.5 | ≥1830 | ≥23 | 75-88 | 9.5-11 | 750 | 300 | Temp Range | Br Temp Coefficient%℃ | |||
20-100℃ | +0.0156%℃ | ||||||||||||||
100-200℃ | +0.0087%℃ | ||||||||||||||
200-300℃ | +0.0007%℃ | ||||||||||||||
YX-12 | 0.70-0.74 | 7.0-7.4 | 358-390 | 4.5-4.9 | 358-478 | 4.5-6 | 80-103 | 10-13 | 450 | 200 | |||||
YXG-24H | 0.95-1.02 | 9.5-10.2 | 692-764 | 8.7-9.6 | ≥1990 | ≥25 | 175-191 | 22-24 | 800 | 350 | -0.025 | -0.20 | |||
YXG-26H | 1.02-1.05 | 10.2-10.5 | 748-796 | 9.4-10.0 | ≥1990 | ≥25 | 191-207 | 24-26 | 800 | 350 | -0.030 | -0.20 | |||
YXG-28H | 1.03-1.08 | 10.3-10.8 | 756-812 | 9.5-10.2 | ≥1990 | ≥25 | 207-220 | 26-28 | 800 | 350 | -0.035 | -0.20 | |||
YXG-30H | 1.08-1.10 | 10.8-11.0 | 788-835 | 9.9-10.5 | ≥1990 | ≥25 | 220-240 | 28-30 | 800 | 350 | -0.035 | -0.20 | |||
YXG-32H | 1.10-1.13 | 11.0-11.3 | 812-860 | 10.2-10.8 | ≥1990 | ≥25 | 230-255 | 29-32 | 800 | 350 | -0.035 | -0.20 | |||
YXG-22 | 0.93-0.97 | 9.3-9.7 | 676-740 | 8.5-9.3 | ≥1433 | ≥18 | 160-183 | 20-23 | 800 | 300 | -0.020 | -0.20 | |||
YXG-24 | 0.95-1.02 | 9.5-10.2 | 692-764 | 8.7-9.6 | ≥1433 | ≥18 | 175-191 | 22-24 | 800 | 300 | -0.025 | -0.20 | |||
YXG-26 | 1.02-1.05 | 10.2-10.5 | 748-796 | 9.4-10.0 | ≥1433 | ≥18 | 191-207 | 24-26 | 800 | 300 | -0.030 | -0.20 | |||
YXG-28 | 1.03-1.08 | 10.3-10.8 | 756-812 | 9.5-10.2 | ≥1433 | ≥18 | 207-220 | 26-28 | 800 | 300 | -0.035 | -0.20 | |||
YXG-30 | 1.08-1.10 | 10.8-11.0 | 788-835 | 9.9-10.5 | ≥1433 | ≥18 | 220-240 | 28-30 | 800 | 300 | -0.035 | -0.20 | |||
YXG-32 | 1.10-1.13 | 11.0-11.3 | 812-860 | 10.2-10.8 | ≥1433 | ≥18 | 230-255 | 29-32 | 800 | 300 | -0.035 | -0.20 | |||
YXG-26M | 1.02-1.05 | 10.2-10.5 | 676-780 | 8.5-9.8 | 955-1433 | 12-18 | 191-207 | 24-26 | 800 | 300 | -0.035 | -0.20 | |||
YXG-28M | 1.03-1.08 | 10.3-10.8 | 676-796 | 8.5-10.0 | 955-1433 | 12-18 | 207-220 | 26-28 | 800 | 300 | -0.035 | -0.20 | |||
YXG-30M | 1.08-1.10 | 10.8-11.0 | 676-835 | 8.5-10.5 | 955-1433 | 12-18 | 220-240 | 28-30 | 800 | 300 | -0.035 | -0.20 | |||
YXG-32M | 1.10-1.13 | 11.0-11.3 | 676-852 | 8.5-10.7 | 955-1433 | 12-18 | 230-255 | 29-32 | 800 | 300 | -0.035 | -0.20 | |||
YXG-24L | 0.95-1.02 | 9.5-10.2 | 541-716 | 6.8-9.0 | 636-955 | 8-12 | 175-191 | 22-24 | 800 | 250 | -0.025 | -0.20 | |||
YXG-26L | 1.02-1.05 | 10.2-10.5 | 541-748 | 6.8-9.4 | 636-955 | 8-12 | 191-207 | 24-26 | 800 | 250 | -0.035 | -0.20 | |||
YXG-28L | 1.03-1.08 | 10.3-10.8 | 541-764 | 6.8-9.6 | 636-955 | 8-12 | 207-220 | 26-28 | 800 | 250 | -0.035 | -0.20 | |||
YXG-30L | 1.08-1.15 | 10.8-11.5 | 541-796 | 6.8-10.0 | 636-955 | 8-12 | 220-240 | 28-30 | 800 | 250 | -0.035 | -0.20 | |||
YXG-32L | 1.10-1.15 | 11.0-11.5 | 541-812 | 6.8-10.2 | 636-955 | 8-12 | 230-255 | 29-32 | 800 | 250 | -0.035 | -0.20 | |||
LTC(YXG-22) | 0.94-0.98 | 9.4-9.8 | 668-716 | 8.4-9.0 | ≥1433 | ≥18 | 167-183 | 21-23 | 840 | 300 | Temp Range | Br Temp Coefficient%℃ | |||
–50-25℃ | ﹢0.005%℃ | ||||||||||||||
20-100℃ | -0.008%℃ | ||||||||||||||
100-200℃ | -0.008%℃ | ||||||||||||||
200-300℃ | -0.011%℃ |
Parameter Name | Unit | SmCo5 | Sm2Co17 |
Density | g/cm³ | 8.2 ~ 8.4 | 8.3 ~ 8.5 |
Curie Temperature | ℃ | 700 ~ 750 | 800 ~ 850 |
Max. Operating Temperature 250 350 | ℃ | 250 | 350 |
Temperature Coefficient Of Br -0.05 -0.03 | %/℃ | -0.05 | -0.03 |
Vickers Hardness 450 ~ 500 550 ~600 | HV | 450 ~ 500 | 550 ~600 |
Electronic Ressistivity | Ω.cm | 5 ~ 6 x 10(-5) | 8 ~ 9 x 10(-5) |
Thermal Conductivity | W/mK | 12 | 13 |
Parameter | Value |
---|---|
Operating Temperature | 250-500°C |
Material | Samarium Cobalt |
Coating | As Customized |
Pull Force | As Customer Requirement |
Corrosion Resistance | High |
Heat Resistance | High |
Application | Spaceflight,National Defense,Microwave,Sensors |
Grade | YX-24H, YX-30H, YXG-28, YXG-30, YXG-32 |
Magnetization | As Customized |
Magnet Type | Ring Magnets Smco Magnet, Samarium Cobalt, Samarium Cobalt Magnet |
1 | Mixing | 1.Mix the ingredients. |
2 | Melting | 2.Dissolve the mixture at high temperature and prepare an alloy. |
3 | Fine pulverization | 3.Turn the alloy into fine powder. |
4 | Molding in a magnetic field | 4.When pressing the fine powder, apply a magnetic field to it and prepare a molded product of powder with aligned directions of magnetization. |
5 | Sintering and heat treatment | 5.Sinter the product at about 1,200℃, and then subject it to heat treatment at about 1000℃ to increase its magnetic characteristics. |
6 | Processing | 6.Process the manufactured magnet base material and finish it into the product shape. |
7 | Magnetization | 7. Surface-treat it for rustproofing |
UNMAG Samarium Cobalt Magnets, made of Smco material, are well known for their excellent corrosion resistance and high temperature resistance, up to 250-500°C. This makes them a perfect choice for high temperature Motors and Generators,military applications,magnetic pump couplings,oil drilling applications,cryogenic applications, spaceflight, national defense, microwave, sensors and other demanding applications.
UNMAG is a leading provider of Samarium Cobalt Magnets, offering a wide range of products with different grades, such as YX-24H, YX-30H, YXG-28, YXG-30, and YXG-32. All our products are manufactured using the highest quality standards in China.
Our Samarium Cobalt Magnets are carefully designed to provide superior performance and reliability. They offer excellent temperature stability, magnetic stability, and superior corrosion resistance, making them ideal for a variety of applications.
At UNMAG, we take pride in providing superior quality Samarium Cobalt Magnets that are designed to meet the demanding requirements of spaceflight, national defense, microwave, sensors and other applications. We strive to consistently provide the highest level of quality and service to our customers.
Brand Name: UNMAG
Place of Origin: China
Application: Spaceflight, National Defense, Microwave, Sensors
Grade: YX-24H, YX-30H, YXG-28, YXG-30, YXG-32
Magnetization: As Customized
Operating Temperature: 250-500°C
Coating: As Customized
We provide high-performance Samarium Cobalt (Sm2Co17) and Samarium Cobalt Magnet with customizations per your requirements.
Samarium Cobalt Magnet Technical Support and Service