Nickel welding wire is a commonly used metal welding material with various brands, such as ERNiCrMo-3, ERNiCrMo-4, ERNiCrMo-13, ERNiCrFe-7 and ERNiCr-3. These wires are widely used in the welding field due to their unique alloy composition and welding properties.
ERNiCrMo-3 is a high-alloy nickel welding wire suitable for welding high-alloy steel and nickel alloys. It has good corrosion resistance and high temperature stability and is commonly used for equipment and pipeline welding in the chemical, petroleum and petrochemical industries.
ERNiCrMo-4 is a nickel-based alloy welding wire suitable for welding stainless steel and nickel-based alloys. It has excellent corrosion resistance and high temperature performance and is commonly used in chemical, marine engineering and nuclear industries.
ERNiCrMo-13 is a high-alloy nickel welding wire commonly used for welding corrosion-resistant alloys, high-temperature alloys and acid-resistant stainless steel. It has excellent corrosion resistance and high temperature strength.
ERNiCrFe-7 is a nickel-iron-based alloy welding wire suitable for welding stainless steel, alloy steel and high-temperature alloys. It has good corrosion resistance and high temperature performance.
ERNiCr-3 is a common nickel welding wire suitable for welding stainless steel, nickel alloys and other high temperature alloys. It is widely used in aerospace, petrochemical, nuclear energy and other fields.
C | Si | Mn | Cr | P | Ni |
≤0.01 | ≤0.2 | ≤0.5 | 22.0-24.0 | ≤0.015 | Rem |
Al | Mo | Fe | Cu | S | Co |
0.10-0.40 | 15.0-16.50 | ≤0.5 | ≤0.1 | <0.01 | <0.20 |
Typical Welding Parameters | |||||
Diameter | Process | Volt | Amps (flat) | Amps (V/OH) | |
inch | (mm) | ||||
0.035 | 0.9 | GMAW | 26-29 | 150-190 | Spray Transfer 100% Argon |
0.045 | 1.2 | GMAW | 28-32 | 180-220 | Spray Transfer 100% Argon |
1/16 | 1.6 | GMAW | 29-33 | 200-250 | Spray Transfer 100% Argon |
1/16 | 1.6 | GTAW | 14-18 | 90-130 | 100% Argon |
3/32 | 2.4 | GTAW | 15-20 | 120-175 | 100% Argon |
1/8 | 3.17 | GTAW | 15-20 | 150-220 | 100% Argon |
Tensile Strength | 109 Ksi | 790 MPA |
Yield Strength | 68 Ksi | 470 MPA |
Elongation | 40-45% | |
Density g/cm3 | 8.60 g/cm3 | |
Melting Point ℃ | 1300-1360℃ | |
Coefficient of Expansion. 21-93 Co, μm/m * Co | 11.90 |
![]() | ![]() |